PLA (standard)
A familiar starting point for models, prototypes and everyday prints at room temperature.
25 product listingsFind the right filament for your next print. Start with the essentials, then explore the settings, properties and sources that matter to you.

Read material selection articles to connect specific grade measurements to loads, part geometry and service conditions.

A familiar starting point for models, prototypes and everyday prints at room temperature.
25 product listings
A practical step up from PLA for tougher functional parts. Expect a little more tuning.
21 product listings
A material to consider for outdoor parts. An enclosed printer is part of the setup.
14 product listings
For flexible parts such as gaskets, protective covers and vibration mounts.
15 product listings
For demanding functional parts where toughness and heat tolerance matter.
9 product listings
A familiar engineering plastic for functional parts, with more demanding printing conditions.
16 product listings83 materials

PLA with a raised melt index and tuned crystallisation so it can be extruded at roughly 24 mm³/s, about 30 % more flow than…
10 product listingsPLA compounded with a chalk-type mineral filler for a diffuse finish; density rises to 1.31–1.38 g/cm³ and flexural strength…
10 product listings
A familiar starting point for models, prototypes and everyday prints at room temperature.
25 product listings
PLA blended with impact modifiers: notched impact strength rises five- to nine-fold while stiffness and tensile strength fall…
11 product listingsPLA regranulated from post-industrial waste; Prusa's own testing shows mechanical parity with virgin PLA, while colour range…
8 product listings
PLA with gloss-forming additives; the finish costs elongation at break, which falls to 2.8 %, and layer adhesion, which in…
15 product listings
PLA with 5–10 wt% chopped carbon fibre: stiffness rises by roughly a third and the surface goes matte black, while tensile…
9 product listingsPLA with 12–20 wt% chopped glass fibre; the Polymaker grade is designed to be annealed, which lifts HDT at 0.45 MPa from 75.5…
2 product listings
PLA with 2–20 wt% phosphorescent additive; both Bambu Lab and Polymaker require a hardened nozzle, and Bambu Lab rules out the…
5 product listings
PLA with a blowing agent. Active-foaming grades expand at the nozzle and reach print densities near 0.40 g/cm³ at reduced flow…
4 product listingsPLA loaded with real metal powder to densities of 1.85–4.0 g/cm³; prints are heavy, polishable and slow to lay down, and the…
6 product listingsPLA blended with polyhydroxyalkanoate, a fermented bio-polyester that colorFabb adds to reduce brittleness; elongation at break…
1 product listingPLA filled with stone or mineral powder — up to 40–50 wt% in Formfutura StoneFil — giving a matte mineral surface at densities…
6 product listings
PLA carrying 10–18 wt% wood powder: it sands and stains like timber, absorbs 1.25 % water — the most of any PLA grade — and…
6 product listings
Semi-crystalline PET with carbon fibre — a genuinely different material from PETG-CF, reaching 182–205 °C heat deflection but…
4 product listings
PETG with chopped carbon fibre: stiffness and heat deflection rise — Prusament reaches 96 °C at 0.45 MPa — while impact…
11 product listingsPETG with a conductive filler for static-dissipative parts; Polymaker's data shows surface resistivity moving three orders of…
2 product listingsGlass-fibre reinforced polyester. The best-documented grade, Polymaker's Fiberon PET-GF15, uses a PET matrix with 15 wt% glass…
3 product listings
A copolyester with more cyclohexanedimethanol than PETG: notched Izod on moulded specimens reaches 93–94 kJ/m² and elongation…
5 product listings
A practical step up from PLA for tougher functional parts. Expect a little more tuning.
21 product listingsPETG regranulated from polyester waste. Prusa's own testing shows a 9 % drop in tensile yield and a 17 % drop in interlayer…
4 product listings
A familiar engineering plastic for functional parts, with more demanding printing conditions.
16 product listingsABS reformulated for lower warping and higher heat: Polymaker's ABS Max reaches Tg 126 °C and 118 °C HDT at 0.45 MPa, against…
4 product listingsABS with chopped carbon fibre: tensile modulus more than doubles to 5210 MPa and warping drops, at the cost of elongation…
7 product listingsABS with a conductive carbon filler bringing surface resistance from above 10¹³ down to 10⁷–10⁹ ohm/sq, the static-dissipative…
4 product listingsABS with a flame-retardant package rated UL 94 V-0 at 1.5 mm on the base resin; the retardant lifts density to 1.18 g/cm³ and…
5 product listingsABS with chopped glass fibre: HDT rises to 99 °C at 0.45 MPa and layer lines blur into a matte finish, while notched Charpy…
4 product listings
Rubber-toughened polystyrene, used mainly as a break-away or d-limonene-soluble support for ABS and ASA; as a model material it…
3 product listings
A material to consider for outdoor parts. An enclosed printer is part of the setup.
14 product listingsASA with chopped carbon fibre: Young's modulus rises from 2450 to 4200 MPa and HDT from 100 to 110 °C, while notched Charpy…
5 product listingsActive-foaming ASA for lightweight outdoor parts: Formfutura's grade activates near 230 °C, peaks between 270 and 285 °C and…
1 product listingASA with 10–15 wt% glass fibre for stiffness and dimensional stability outdoors; ZYLtech requires a hardened nozzle of 0.6 mm…
3 product listings
PC with chopped carbon fibre: flexural modulus rises from about 2.1 to 3.5–6.5 GPa and HDT at 1.8 MPa from 93 to 106 °C, and…
6 product listingsPolycarbonate with a conductive filler bringing surface resistance from above 10¹³ into the 10⁷–10⁹ ohm/sq dissipative band…
1 product listingUL 94 V-0 polycarbonate for electrical enclosures; the retardant roughly halves elongation at break to 2.4–3.5 % and, in Bambu…
4 product listingsPolycarbonate with 30 wt% short glass fibre. Owens Corning's XSTRAND GF30-PC is the reference grade: 5400 MPa tensile modulus…
1 product listingA PC/ABS alloy that keeps most of PC's heat resistance while printing closer to ABS; notched Charpy of 25.8 kJ/m² beats both…
5 product listings
For demanding functional parts where toughness and heat tolerance matter.
9 product listingsBio-based nylon from castor oil, sitting between PA12 and PA6 for moisture. Prusa's grade posts an interlayer adhesion of 32…
1 product listingThe long-chain nylon: fewest amide groups, so the least moisture uptake and the best dimensional stability of the family —…
3 product listingsThe toughest and most abrasion-resistant common nylon, and the most moisture-hungry: it must be printed dry, in an enclosure…
3 product listingsA PA6/66 copolymer that prints more easily than straight PA6. Polymaker publishes full dry and wet printed blocks for it: at…
4 product listingsHigher-melting than PA6 and common as an injection-moulding resin, but effectively absent from the filament market — no…
0 product listingsSemi-aromatic nylon: aromatic diacid units lift the melting point to about 231 °C and the whole family is sold on lower…
1 product listingAramid-reinforced polyamide. No aramid-filled nylon filament was found in any catalogue searched — every aramid filament on the…
0 product listings
Carbon-fibre nylon on a PA12 matrix, chosen for humidity stability rather than peak strength: 1.5 % equilibrium moisture…
4 product listingsA stiff, reinforced engineering material for brackets, tooling and loaded parts.
6 product listingsStatic-dissipative carbon-filled nylon for electronics tooling. Strong in plane at 84 MPa but only 21.5 MPa in Z — a quarter of…
1 product listingGlass-fibre PA12: 7.8 GPa tensile modulus with 4.5 % elongation at break, nearly double the ductility of glass-filled PA6, and…
3 product listings
Glass-fibre PA6: modulus to 5.4 GPa and HDT to 191 °C, and the thirstiest material in the whole dataset at 3.33 % equilibrium…
6 product listings
Long-chain carbon-fibre nylon reaching 194 °C HDT at 0.45 MPa and 170 °C at 1.8 MPa, with saturated moisture uptake of 0.88 % —…
2 product listingsCarbon-fibre semi-aromatic nylon: 10–15 wt% chopped fibre in a PPA matrix reaches 188–227 °C HDT at 0.45 MPa and takes up about…
7 product listingsCarbon-filled hard TPU at 70 Shore D for damping mounts and semi-rigid brackets. Extrudr flags it as the one FLEX grade that…
1 product listingTPU with a blowing agent, sold as varioShore, Filaflex Foamy, TPU-Aero and TPU Air: foaming starts near 230 °C and the printed…
6 product listings
Below 85 Shore A the filament will not push through anything but a short constrained direct-drive path. Fiberlogy's 81 Shore A…
4 product listingsA styrenic rubber rather than a polyurethane: it needs no drying at all, prints at 260–280 °C and 10–30 mm/s, and trades TPU's…
2 product listings
Genuinely rubbery TPU at 82–85 Shore A with 650 % elongation and a tensile modulus of 12–22 MPa. Direct drive only, 15–40 mm/s…
6 product listings
For flexible parts such as gaskets, protective covers and vibration mounts.
15 product listings
The rigid end of the TPU range at 98 Shore A to 60 Shore D: it prints almost like a rigid filament, runs on Bowden, and posts…
3 product listingsA flexible polyamide blend used in cushioning, footwear and sports equipment.
1 product listingCarbon-fibre polypropylene: HDT jumps to 158 °C at 0.45 MPa while density stays at 0.91 g/cm³, the best stiffness-to-weight in…
3 product listingsGlass-fibre polypropylene: filament tensile yield of 46.6 MPa, more than double the carbon-fibre grade, at the cost of density…
3 product listingsNon-polar, chemically inert and effectively non-hygroscopic. One brand — Spectrum's low-warp HDPE — carries the whole retail…
1 product listing
The lightest common filament at 0.91 g/cm³ and effectively non-hygroscopic at 0.04 % uptake, with unbeatable living-hinge…
4 product listingsAcrylic filament sold as a transparent alternative to PC. Only one supplier listing was obtainable and it publishes no…
1 product listingThe classic gear and bearing plastic, and still all but absent from the filament market: no POM filament appears in 3DJAKE's…
0 product listingsA fluoropolymer with outstanding chemical and UV resistance at 1.71 g/cm³ and $251/kg. The only material in the dataset with a…
1 product listingPEEK with short carbon or glass fibre. Carbon roughly doubles tensile modulus to 8100 MPa and cuts thermal expansion to about a…
5 product listingsFilled PPS reaches 252 °C heat deflection at 0.45 MPa and Polymaker states its grade needs no heated chamber — the one way into…
5 product listingsThe benchmark high-temperature engineering polymer: 60-100 MPa printed tensile, Tg 143-151 °C, melting 343 °C, UL 94 V-0 and…
5 product listingsThe highest heat deflection in the dataset — 215 °C at 1.8 MPa on printed Stratasys coupons — and the most demanding process: a…
6 product listingsThe aircraft-interior PEI: UL 94 V-0 plus a documented flame, smoke and toxicity pedigree, HDT 178 °C at 0.45 MPa, and the…
6 product listingsAmorphous PEKK avoids PEEK's crystallisation-control problem and prints at a lower chamber temperature. Unfilled grades give…
6 product listingsSemi-crystalline, melting at 280-283 °C, UL 94 V-0 and resistant to essentially every solvent below 200 °C. Unusually ductile…
3 product listingsTg 230 °C, the highest glass transition here, and repeatedly steam-autoclavable — the usual choice for sterilisable tooling…
4 product listingsThe entry point to the sulfones at $250/kg: Tg 185-187 °C against PPSU's 230 °C, but 8 % printed elongation against 3 %, so it…
1 product listingSupport that peels off by hand rather than dissolving, avoiding PVA's moisture handling. Polymaker publishes an adhesion matrix…
4 product listingsA vinyl alcohol copolymer that dissolves faster and in cooler water than straight PVA, and bonds to a wider range of model…
1 product listingBreak-away support compounded to survive a PEEK or PEI build: Tg 225 °C, where PVA and PLA-based supports would decompose.…
4 product listingsThe standard water-soluble support for PLA, TPU, PVB and PETG. At 10.21 % equilibrium water absorption it is by a wide margin…
5 product listings
PLA loaded with conductive carbon to give volume conductivity rather than the merely dissipative range of ESD grades. The…
4 product listingsIron-filled PLA at about 1.85 g/cm³ that responds to magnets and behaves like pure iron. Slow to print at 20–30 mm/s, brittle…
1 product listingPrints close to PLA and smooths to a layer-free surface with isopropyl alcohol rather than a hot solvent — the only common…
3 product listingsTry a broader name or clear the family filter.