3D Printing Info
ASA · Material guide

Glass-fibre ASA (ASA-GF)

ASA with 10–15 wt% glass fibre for stiffness and dimensional stability outdoors; ZYLtech requires a hardened nozzle of 0.6 mm or larger and Spectrum recommends ruby or hardened.

3 product listings3 brands
Open in interactive comparison
Understand the material

At a glance

Before you print

Setup difficulty
Intermediate — dry filament and a tuned profile; ZYLtech requires a hardened nozzle of 0.6 mm or larger
Nozzle wear
Highly abrasive — standard GF composite
Read conditions and sources ↓
Read the full material overview

ASA with 10–15 wt% glass fibre for stiffness and dimensional stability outdoors; ZYLtech requires a hardened nozzle of 0.6 mm or larger and Spectrum recommends ruby or hardened.

Applications

ASA-GF is an outdoor rigidity material for manufacturing tools, housings, covers and exposed mechanical parts. Spectrum lists these uses for ASA-X GF10, connecting glass reinforcement with stiffness and the ASA matrix with resistance to prolonged sunlight and moisture. It fits parts that need to retain a locating or mounting shape rather than act as elastic hinges.

The grade and specimen type matter. Spectrum’s published mechanical and thermal figures include injection-molded specimens, so they are not direct load ratings for a printed bracket. ZYLtech reports limited elongation for its grade, favoring generous roots and distributed loads over narrow flexures. Reinforcement content and required nozzle size differ between manufacturers, even when both products are called ASA-GF.

  • Manufacturing tools and equipment ↗

    FDM · Spectrum ASA-X GF10; 10% glass fibre · Manufacturer-listed applications

    Spectrum lists manufacturing tools and equipment for ASA-X GF10. Stiffness and outdoor stability are the intended advantages; its molded-specimen data do not directly establish the strength of an FDM tool.

  • Housings and covers exposed outdoors ↗

    FDM · Spectrum ASA-X GF10 · Manufacturer-listed applications

    Spectrum lists housings, covers and components requiring high outdoor-exposure resistance. This is a manufacturer-listed use for the exact grade rather than a documented installed enclosure.

Sources
Find printable models

Check the model’s material and process notes before choosing a filament.

Plan your printer setup

Printing quick reference

All print settings ↓

Representative catalog values. Check the exact grade and its linked conditions before using a setting.

04

Drying

—

Full value & sources

—

—
Go deeper when you need to

Properties & source data

60 documented fields

Open a topic to explore the complete data. Each value keeps its original conditions, units and dated sources.

Material & market8 fields
Glass-fibre ASA (ASA-GF) — Identity & Market
Property and unitPublished value and conditionsSources and dates
Base polymer / chemistryASA reinforced with chopped glass fibre — 10 wt% (Spectrum ASA-X GF10), 15 wt% (ZYLtech ASA-GF)
2 sources
Density (g/cm³)1.07 (ZYLtech) and 1.11 (Spectrum), ISO 1183
2 sources
Typical price (USD/kg)1 kg spools cluster near 28
2 sources
Price range across brands (USD/kg)27–34 across brands; Ambrosia 27, ZYLtech 30, Siraya Tech 34
3 sources
Market availability (1–5)Niche, a handful of specialist brands
3 sources
Spool sizes & diameters1.75 and 2.85 mm; 1 kg spools
2 sources
Typical applicationsOutdoor brackets and mounts that need stiffness and dimensional stability under sun and moisture
2 sources
Diameter tolerance (± mm)±0.01 at 95 % probability and ±0.02 at 100 % (ZYLtech)
1 source
Print settings11 fields
Glass-fibre ASA (ASA-GF) — Printing Parameters
Property and unitPublished value and conditionsSources and dates
Nozzle temperature (°C)240–270 (Spectrum); 240–280 (ZYLtech)
2 sources
Bed temperature (°C)80–100 (Spectrum); 90–110 on PEI (ZYLtech)
2 sources
Enclosure / chamber requirement (1–5)Enclosure recommended
1 source
Part cooling fan0–20 % (Spectrum)
1 source
Bed surface & adhesion aidPEI sheet, BuildTak or an adhesion aid such as Magigoo (Polymaker); Simplify3D also lists Kapton tape and ASA slurry
2 sources
Maximum volumetric flow (mm³/s; see test conditions) (mm³/s)2.4–5.6 at Spectrum's 30–70 mm/s on a 0.4 mm nozzle at 0.2 mm layer; ZYLtech allows up to 200 mm/s
3 sources
Warping tendency (1–5)Moderate — needs adhesion aid or draught shield
1 source
Bed-adhesion difficulty (1–5)Needs a specific surface plus adhesive
1 source
Stringing / oozing tendency (1–5)Slight — Polymaker advises 1–2 mm retraction at 20–30 mm/s
1 source
Overall printing difficulty (1–5)Intermediate — dry filament and a tuned profile; ZYLtech requires a hardened nozzle of 0.6 mm or larger
2 sources
Extruder requirementZYLtech specifies a hardened nozzle 0.6 mm or larger; Spectrum bases its settings on a 0.5 mm nozzle
2 sources
Nozzle wear & reliability5 fields
Glass-fibre ASA (ASA-GF) — Hardware Wear & Reliability
Property and unitPublished value and conditionsSources and dates
Nozzle hardness required (1–4)Hardened steel required — Spectrum recommends ruby or hardened, ZYLtech requires hardened
2 sources
Abrasiveness (1–5)Highly abrasive — standard GF composite
2 sources
Nozzle clog risk (1–5)Moderate — needs dry filament and a clean nozzle; Prusa lists higher risk of nozzle clogging for glass-filled composites
1 source
Heat-creep / jam sensitivity (1–5)Slightly sensitive
1 source
Hotend requirementNo special hotend required
1 source
Moisture & drying4 fields
Glass-fibre ASA (ASA-GF) — Moisture Behaviour
Property and unitPublished value and conditionsSources and dates
Moisture absorption (hygroscopicity) (1–5)Moderate — the ASA matrix takes up 0.40–0.45 % saturated at 25 °C / 55 % RH; no glass-filled grade publishes its own figure
3 sources
Symptoms when wetBubbling and popping at the nozzle, stringing and a rough surface
1 source
Effect of moisture on strengthNo dry-versus-conditioned figures are published; Polymaker groups the styrenics as moderate-sensitivity and absorbed water shows as bubbling and poor layer adhesion
1 source
Storage requirementSealed with desiccant; Polymaker rates the styrenics moderate-sensitivity
1 source
Strength & mechanical properties10 fields
Glass-fibre ASA (ASA-GF) — Mechanical Properties
Property and unitPublished value and conditionsSources and dates
Tensile strength (XY) (MPa)33–36 at break, ISO 527 (ZYLtech; specimen type not stated); Spectrum quotes 55 at break on injection-moulded specimens
2 sources
Young's modulus (MPa)2540–2890 (ZYLtech; specimen type not stated) and 2550 (Spectrum, injection-moulded), ISO 527
2 sources
Elongation at break (%)3.4 at break (ZYLtech; specimen type not stated); Spectrum quotes 2.80 at yield on injection-moulded specimens
2 sources
Flexural modulus (MPa)2130–2480 flexural modulus, ISO 178 (ZYLtech; specimen type not stated)
1 source
Charpy impact, notched (kJ/m²)8.3 notched Charpy at 23 °C on injection-moulded specimens (Spectrum, ISO 179-1eA); ZYLtech publishes notched Izod 6.9 by ISO 180 instead
2 sources
Other impact dataCharpy unnotched 25 kJ/m² at 23 °C on injection-moulded specimens (Spectrum, ISO 179-1eU); ZYLtech notched Izod 6.9 kJ/m² (ISO 180)
2 sources
Brittleness (1–5)Brittle — snaps with little warning; elongation at break 3.4 %
1 source
Creep resistance / sustained load (1–5)Good — no creep test found; chopped glass fibre lifts modulus to 2540–2890 against 2379–2450 for unfilled ASA
3 sources
Fatigue / repeated-flex resistance (1–5)Below average — no GF-grade S-N curve; elongation at break falls to 3.4 % against 6.7–9.2 % for unfilled ASA
3 sources
Elasticity / flexibility (1–5)Rigid
1 source
Heat & temperature5 fields
Glass-fibre ASA (ASA-GF) — Thermal Properties
Property and unitPublished value and conditionsSources and dates
HDT at 0.45 MPa (°C)100 (Spectrum, injection-moulded, ISO 75 at 0.45 MPa)
1 source
HDT at 1.8 MPa (°C)97–99 unannealed (ZYLtech, ISO 75 at 1.8 MPa; specimen type not stated); Spectrum 90 on injection-moulded specimens
2 sources
Melting point / Vicat (°C)Amorphous ASA matrix; Vicat 98 (Spectrum, ISO 306). ZYLtech quotes a 210–220 °C melting range by ISO 11357 for its grade
2 sources
Continuous service temperature (°C)93 — Prusa publishes this as the temperature resistance of Prusament ASA
1 source
Flammability / UL 94Flammable; no UL 94 rating published
1 source
Weather & chemical resistance5 fields
Glass-fibre ASA (ASA-GF) — Environment & Chemical
Property and unitPublished value and conditionsSources and dates
UV resistance (1–5)Excellent — designed for permanent outdoor use; Spectrum states the parts resist prolonged UV and moisture exposure
2 sources
Chemical resistanceGood against weak acids, weak alkalis, oils and grease; dissolved by acetone
1 source
Food contactNot food safe
1 source
Biodegradability / compostabilityNot biodegradable
1 source
RecyclabilityNot accepted in household plastic collection
1 source
Health & safety4 fields
Glass-fibre ASA (ASA-GF) — Health & Safety
Property and unitPublished value and conditionsSources and dates
Fume toxicity (1–5)High — hazardous VOC such as styrene; enclosure and filtration needed
2 sources
Hazardous species emittedStyrene. Bambu Lab states ABS and ASA release harmful gases such as styrene at printing temperature, which can be toxic and cause dizziness or nausea. Azimi et al. measured styrene from every styrenic filament tested but did not test ASA itself
2 sources
Ventilation / filtration requirement (1–5)Enclosure with carbon and HEPA filtration
2 sources
Dust & fibre handling hazardGlass fibre is bound in the matrix; avoid inhaling sanding dust
1 source
Finishing & post-processing5 fields
Glass-fibre ASA (ASA-GF) — Post-Processing
Property and unitPublished value and conditionsSources and dates
Sanding & machiningSands well and takes filler before painting
1 source
Painting & finishingPaints readily; ASA holds colour outdoors so many parts are left unpainted
1 source
Gluing & solvent weldingSolvent-welds with acetone
1 source
Vapour / chemical smoothingAcetone vapour smoothing works
1 source
Support material pairingHIPS breaks away or dissolves in d-limonene; Bambu Lab sells a Support for ABS that also serves ASA
1 source
Solvents & solubility3 fields
Glass-fibre ASA (ASA-GF) — Solvents & Solubility
Property and unitPublished value and conditionsSources and dates
Soluble inAcetone dissolves the resin and leaves the fibre; MEK, THF, ethyl acetate and chlorinated solvents attack the styrenic backbone.
2 sources
Softened or crazed byLimonene attacks some grades — Prusa reports Prusament ASA Orange flaking apart as layer adhesion fails.
1 source
Solvent welding & smoothing agentAcetone vapour reaches only the resin fraction, so the fibre is left standing proud of the smoothed surface.
2 sources
How to read these values

Values describe representative grades, not every spool. Manufacturer datasheets and independent tests retain their source labels and dates. Printed orientation, test method, conditioning and formulation can change results. Unknown values are —. A listed use is not a certification. Shore A, Shore D and Rockwell hardness are separate scales.

Find a specific filament

Product listings and datasheets

3 listings

Historical USD/kg snapshots. Read each listing’s sale/from qualifiers, spool mass, source date, shipping and tax notes. Product figures are separate from the material summary.

Browse 3 products from 3 brands
AmbrosiaASA-GF26.99 USD/kg

$26.99 / 1 kg spool; $44.99 for the 2 kg variant = $22.50/kg, filastruder.com, Aug 2026

Handle ambrosia-asa-gf-glass-filled-filament. Ambrosia's specification table for ASA-GF lists density and all mechanical values as TBD; only HDT is given, as 88 °C or above (also marked TBD).

Open product listing ↗
Ambrosia ASA-GF — product-specific figures
Spool sizes & diameters1 kg and 2 kg spools, 130 g spool weight; 1.75 mm
Diameter tolerance (± mm)0.03
Nozzle temperature (°C)250–280 (Ambrosia recommends 270)
Bed temperature (°C)100–120 (Ambrosia recommends 110)
Recommended chamber temperature (°C)40–120 (Ambrosia recommends 45)
Part cooling fan0–70 %, depending on cooling capability
ZYLtechASA-GF (Glass Fiber)29.95 USD/kg

$29.95 / 1 kg spool at 1.75 mm, zyltech.com, Aug 2026 (quantity breaks to $28.45)

15 wt% glass fibre, made in Houston. ZYLtech requires a hardened nozzle and suggests 0.6 mm.

Open product listing ↗
ZYLtech ASA-GF (Glass Fiber) — product-specific figures
Density (g/cm³)1.07 (ISO 1183)
Diameter tolerance (± mm)±0.02
Nozzle temperature (°C)240–280
Bed temperature (°C)90–110 on PEI
Maximum volumetric flow (mm³/s; see test conditions) (mm³/s)up to 20 (manufacturer maximum flow rate)
Tensile strength (XY) (MPa)33–36 at break (ISO 527)
Young's modulus (MPa)2540–2890 (ISO 527)
Elongation at break (%)3.4 at break (ISO 527)
Flexural modulus (MPa)2130–2480 (ISO 178)
Other impact dataIzod notched 6.9 kJ/m² at 23 °C (ISO 180)
HDT at 1.8 MPa (°C)97–99 unannealed (ISO 75, 1.8 MPa)
Melting point / Vicat (°C)210–220 melting (ISO 11357)
Siraya TechFibreheart ASA-GF33.99 USD/kg

$33.99 / 1 kg spool, siraya.tech US store, Aug 2026 (list $39.99)

10 % chopped glass fibre. Hardened steel nozzle of 0.4 mm or larger specified.

Open product listing ↗
Siraya Tech Fibreheart ASA-GF — product-specific figures
Density (g/cm³)1.1 (ISO 1183)
Nozzle temperature (°C)250-270
Bed temperature (°C)100-110
Recommended chamber temperature (°C)60-80 (vendor recommended enclosure temperature)
Tensile strength (XY) (MPa)47.5 (printed XY, ISO 527)
Young's modulus (MPa)2993 (ASTM D638)
Elongation at break (%)3.1 (printed XY, ASTM D638)
Flexural strength (MPa)81 (flexural, standard not stated)
Flexural modulus (MPa)2810 (flexural, standard not stated)
Charpy impact, notched (kJ/m²)8 (Charpy, standard not stated)
Hardness (scale-specific) (Shore A / Shore D / Rockwell)81 Shore D (ISO 7619)
HDT at 0.45 MPa (°C)98 (method B, 0.45 MPa)
HDT at 1.8 MPa (°C)94 (method A, 1.8 MPa)
Glass transition (Tg) (°C)106

Compare Glass-fibre ASA (ASA-GF) with another filament