Filament comparison
ASA-GF vs PETG-GF
Compare printing settings, strength, heat resistance, dated prices and sources.
2 selected · all documented properties
| Property | Glass-fibre ASA (ASA-GF)ASA | Glass-fibre polyester (PETG-GF / PET-GF)PETG |
|---|---|---|
| Market snapshot | ||
| Listing priceUSD/kg; dated snapshots | $29.95/kg median; $26.99–$33.99/kg across 3 dated product listings | $27.38/kg median; $18.99–$29.99/kg across 3 dated product listings |
| Identity & Market | ||
| Base polymer / chemistry | ASA reinforced with chopped glass fibre — 10 wt% (Spectrum ASA-X GF10), 15 wt% (ZYLtech ASA-GF)[1][2] | Glass-fibre reinforced polyester. Polymaker's Fiberon PET-GF15 uses a PET rather than a PETG matrix and carries 15 wt% glass fibre[3] |
| Densityg/cm³ | 1.07 (ZYLtech) and 1.11 (Spectrum), ISO 1183[1][2] | 1.43 (Fiberon PET-GF15, ISO 1183)[3] |
| Typical priceUSD/kg | 1 kg spools cluster near 28[4][5] | 1 kg spools cluster near 25[6][7] |
| Price range across brandsUSD/kg | 27–34 across brands; Ambrosia 27, ZYLtech 30, Siraya Tech 34[4][5][8] | 19–30 across brands; ELEGOO 19, Polymaker Fiberon 30[6][7] |
| Market availability1–5 | Niche, a handful of specialist brands[4][1][2] | Niche, a handful of specialist brands[6][7] |
| Spool sizes & diameters | 1.75 and 2.85 mm; 1 kg spools[2][4] | 1.75 mm; 0.5 and 1 kg spools[7] |
| Typical applications | Outdoor brackets and mounts that need stiffness and dimensional stability under sun and moisture[1][2] | Stiff, dimensionally stable fixtures; the Fiberon grade is designed to be annealed for heat resistance[3] |
| Diameter tolerance± mm | ±0.01 at 95 % probability and ±0.02 at 100 % (ZYLtech)[2] | Not documented |
| Printing Parameters | ||
| Nozzle temperature°C | 240–270 (Spectrum); 240–280 (ZYLtech)[1][2] | Not documented |
| Bed temperature°C | 80–100 (Spectrum); 90–110 on PEI (ZYLtech)[1][2] | Not documented |
| Enclosure / chamber requirement1–5 | Enclosure recommended[9] | Not documented |
| Part cooling fan | 0–20 % (Spectrum)[1] | Not documented |
| Bed surface & adhesion aid | PEI sheet, BuildTak or an adhesion aid such as Magigoo (Polymaker); Simplify3D also lists Kapton tape and ASA slurry[10][11] | Textured PEI, satin or powder-coated sheets; on smooth PEI a glue stick acts as a release agent[12][13] |
| Maximum volumetric flow (mm³/s; see test conditions)mm³/s | 2.4–5.6 at Spectrum's 30–70 mm/s on a 0.4 mm nozzle at 0.2 mm layer; ZYLtech allows up to 200 mm/s[1][2][14] | Not documented |
| Warping tendency1–5 | Moderate — needs adhesion aid or draught shield[9] | Not documented |
| Bed-adhesion difficulty1–5 | Needs a specific surface plus adhesive[10] | Needs the right surface or a thin adhesive — the problem is releasing the part, not sticking it[12][13] |
| Stringing / oozing tendency1–5 | Slight — Polymaker advises 1–2 mm retraction at 20–30 mm/s[10] | Moderate — retraction tuning needed; Polymaker names stringing as PETG's common quirk[13] |
| Overall printing difficulty1–5 | Intermediate — dry filament and a tuned profile; ZYLtech requires a hardened nozzle of 0.6 mm or larger[2][1] | Not documented |
| Extruder requirement | ZYLtech specifies a hardened nozzle 0.6 mm or larger; Spectrum bases its settings on a 0.5 mm nozzle[2][1] | Not documented |
| Hardware Wear & Reliability | ||
| Nozzle hardness required1–4 | Hardened steel required — Spectrum recommends ruby or hardened, ZYLtech requires hardened[1][2] | Hardened steel required[3] |
| Abrasiveness1–5 | Highly abrasive — standard GF composite[1][2] | Highly abrasive — standard GF composite[3] |
| Nozzle clog risk1–5 | Moderate — needs dry filament and a clean nozzle; Prusa lists higher risk of nozzle clogging for glass-filled composites[15] | Moderate — needs dry filament and a clean nozzle; Prusa lists higher risk of nozzle clogging for glass-filled composites[15] |
| Heat-creep / jam sensitivity1–5 | Slightly sensitive[11] | Slightly sensitive[16] |
| Hotend requirement | No special hotend required[11] | No special hot-end required[16] |
| Moisture Behaviour | ||
| Moisture absorption (hygroscopicity)1–5 | Moderate — the ASA matrix takes up 0.40–0.45 % saturated at 25 °C / 55 % RH; no glass-filled grade publishes its own figure[17][18][19] | Moderate (0.3–0.8 %) — the PETG matrix reaches 0.40 % saturated at 25 °C / 55 % RH; no glass-filled grade publishes its own figure[12] |
| Symptoms when wet | Bubbling and popping at the nozzle, stringing and a rough surface[20] | Bubbling and popping at the nozzle, stringing and a rough surface[20] |
| Effect of moisture on strength | No dry-versus-conditioned figures are published; Polymaker groups the styrenics as moderate-sensitivity and absorbed water shows as bubbling and poor layer adhesion[20] | Polymaker groups PETG with nylon, PVA and TPU as highly hygroscopic; no dry-versus-conditioned strength figures are published for this grade and the loss shows as bubbling and poor layer adhesion[20] |
| Storage requirement | Sealed with desiccant; Polymaker rates the styrenics moderate-sensitivity[20] | Sealed with desiccant; Polymaker groups PETG with the highly hygroscopic materials[20][13] |
| Mechanical Properties | ||
| Tensile strength (XY)MPa | 33–36 at break, ISO 527 (ZYLtech; specimen type not stated); Spectrum quotes 55 at break on injection-moulded specimens[2][1] | 59.9 ± 0.8 printed XY, ISO 527 (Fiberon PET-GF15)[3] |
| Young's modulusMPa | 2540–2890 (ZYLtech; specimen type not stated) and 2550 (Spectrum, injection-moulded), ISO 527[2][1] | 4144 ± 133 printed XY, ISO 527 (Fiberon PET-GF15)[3] |
| Elongation at break% | 3.4 at break (ZYLtech; specimen type not stated); Spectrum quotes 2.80 at yield on injection-moulded specimens[2][1] | 4.0 ± 0.5 printed XY, ISO 527 (Fiberon PET-GF15)[3] |
| Flexural strengthMPa | Not documented | 104.2 ± 2.4 printed XY, ISO 178 (Fiberon PET-GF15)[3] |
| Flexural modulusMPa | 2130–2480 flexural modulus, ISO 178 (ZYLtech; specimen type not stated)[2] | 3705 ± 85 printed XY, ISO 178 (Fiberon PET-GF15)[3] |
| Charpy impact, notchedkJ/m² | 8.3 notched Charpy at 23 °C on injection-moulded specimens (Spectrum, ISO 179-1eA); ZYLtech publishes notched Izod 6.9 by ISO 180 instead[1][2] | 8.7 ± 0.6 printed XY, ISO 179, notched (Fiberon PET-GF15)[3] |
| Other impact data | Charpy unnotched 25 kJ/m² at 23 °C on injection-moulded specimens (Spectrum, ISO 179-1eU); ZYLtech notched Izod 6.9 kJ/m² (ISO 180)[1][2] | Charpy unnotched 27.2 ± 2.0 printed XY (Fiberon PET-GF15, ISO 179)[3] |
| Layer adhesion / Z tensileMPa | Not documented | 48.2 ± 0.3 printed Z, ISO 527 (Fiberon PET-GF15)[3] |
| Brittleness1–5 | Brittle — snaps with little warning; elongation at break 3.4 %[2] | Brittle — snaps with little warning; elongation 4.0 % in XY and 2.6 % in Z[3] |
| Creep resistance / sustained load1–5 | Good — no creep test found; chopped glass fibre lifts modulus to 2540–2890 against 2379–2450 for unfilled ASA[2][18][17] | Below average — no GF-grade creep test; the CF grades sagged to 14.8–16.7 mm over 5 days at 1.25 kg against 17.1–20.4 mm unfilled[21][22][23] |
| Fatigue / repeated-flex resistance1–5 | Below average — no GF-grade S-N curve; elongation at break falls to 3.4 % against 6.7–9.2 % for unfilled ASA[2][18][17] | Below average — no GF-grade S-N curve; elongation at break falls to 4.0 % in XY against 5.2–9.3 % unfilled[3][24] |
| Elasticity / flexibility1–5 | Rigid[2] | Rigid[3] |
| Z strength as % of XY% | Not documented | 80 (Fiberon PET-GF15, printed Z against XY tensile)[3] |
| Thermal Properties | ||
| HDT at 0.45 MPa°C | 100 (Spectrum, injection-moulded, ISO 75 at 0.45 MPa)[1] | 81.6 as printed, 133.7 after annealing (ISO 75, 0.45 MPa)[3] |
| HDT at 1.8 MPa°C | 97–99 unannealed (ZYLtech, ISO 75 at 1.8 MPa; specimen type not stated); Spectrum 90 on injection-moulded specimens[2][1] | 71.8 as printed, 87.3 after annealing (ISO 75, 1.8 MPa)[3] |
| Glass transition (Tg)°C | Not documented | 59.5 (DSC)[3] |
| Melting point / Vicat°C | Amorphous ASA matrix; Vicat 98 (Spectrum, ISO 306). ZYLtech quotes a 210–220 °C melting range by ISO 11357 for its grade[1][2] | 231.6 melting (DSC); Vicat 232.6 (ISO 306)[3] |
| Continuous service temperature°C | 93 — Prusa publishes this as the temperature resistance of Prusament ASA[25] | Not documented |
| Annealing response | Not documented | Annealing lifts HDT at 0.45 MPa from 81.6 to 133.7 °C[3] |
| Thermal expansion (CTE)µm/m·K | Not documented | 20 along the print bead and 63–74 in the build direction at 30 °C (30 wt% GF, large-format printed, TMA)[26] |
| Flammability / UL 94 | Flammable; no UL 94 rating published[17] | UL 94 HB at 1.5 mm (Fiberon PET-GF15)[3] |
| Environment & Chemical | ||
| UV resistance1–5 | Excellent — designed for permanent outdoor use; Spectrum states the parts resist prolonged UV and moisture exposure[1][27] | Not documented |
| Chemical resistance | Good against weak acids, weak alkalis, oils and grease; dissolved by acetone[18] | Withstands acids, alkalis, oils and UV exposure[13] |
| Food contact | Not food safe[10] | Not certified for food contact as filament[13] |
| Biodegradability / compostability | Not biodegradable[10] | Not biodegradable[13] |
| Recyclability | Not accepted in household plastic collection[10] | Not accepted in household plastic collection[13] |
| Electrical & ESD properties | Not documented | Surface resistivity above 10¹² ohm — insulating (Fiberon PET-GF15, ANSI/ESD S11.11)[3] |
| Health & Safety | ||
| Fume toxicity1–5 | High — hazardous VOC such as styrene; enclosure and filtration needed[28][9] | Moderate — measurable VOCs and UFPs, ventilation advised[28] |
| Hazardous species emitted | Styrene. Bambu Lab states ABS and ASA release harmful gases such as styrene at printing temperature, which can be toxic and cause dizziness or nausea. Azimi et al. measured styrene from every styrenic filament tested but did not test ASA itself[9][28] | Not documented |
| Ventilation / filtration requirement1–5 | Enclosure with carbon and HEPA filtration[28][9] | Open a window / occasional ventilation[28] |
| Dust & fibre handling hazard | Glass fibre is bound in the matrix; avoid inhaling sanding dust[1] | Glass fibre is bound in the matrix; avoid inhaling sanding dust[3] |
| Post-Processing | ||
| Sanding & machining | Sands well and takes filler before painting[10] | Sands poorly — the material is tough and gums rather than powders[16] |
| Painting & finishing | Paints readily; ASA holds colour outdoors so many parts are left unpainted[10] | Not documented |
| Gluing & solvent welding | Solvent-welds with acetone[18] | Cyanoacrylate; no common solvent welds PETG cleanly[16] |
| Vapour / chemical smoothing | Acetone vapour smoothing works[18] | No practical vapour smoothing[16] |
| Support material pairing | HIPS breaks away or dissolves in d-limonene; Bambu Lab sells a Support for ABS that also serves ASA[9] | Prints its own supports; Polymaker rates PolyDissolve S1 for PETG[16] |
| Solvents & Solubility | ||
| Soluble in | Acetone dissolves the resin and leaves the fibre; MEK, THF, ethyl acetate and chlorinated solvents attack the styrenic backbone.[29][18] | No common workshop solvent; dichloromethane — a carcinogen — dissolves the matrix surface, 1,2-dichloroethane destroys it in a week.[30][31] |
| Softened or crazed by | Limonene attacks some grades — Prusa reports Prusament ASA Orange flaking apart as layer adhesion fails.[32] | Acetone (+16 % weight over 1 year at 23 °C), ethyl acetate, toluene and DMF swell and soften it; methanol crazes it.[30] |
| Solvent welding & smoothing agent | Acetone vapour reaches only the resin fraction, so the fibre is left standing proud of the smoothed surface.[31][18] | Dichloromethane reaches only the resin, so the fibre is left standing proud of the surface. Controlled carcinogen.[31] |
Material entries describe families or representative grades, not an interchangeable specification for every spool. Test methods, orientations and conditions may differ. Unknown values are marked “Not documented”. Prices and source dates remain historical snapshots; check the linked guide for product details. Differences highlight text, not a universal winner.
Sources for this comparison
- Spectrum ASA-X GF10 Technical Data Sheet (mechanical and thermal data marked injection-moulded) Spectrum Filaments · 2026-08 · tds
- ZYLtech ASA-GF Filament Technical Data Sheet v1 ZYLtech · 2026-08 · tds
- Fiberon PET-GF15 Technical Data Sheet V1.0 Polymaker · 2026-08 · tds
- Filastruder product catalogue Filastruder · 2026-08 · vendor
- ZYLtech ASA-GF Glass Fiber filament — product page ZYLtech · 2026-08 · vendor
- ELEGOO product catalogue ELEGOO · 2026-08 · vendor
- Polymaker product catalogue Polymaker · 2026-08 · vendor
- Siraya Tech Fibreheart ASA-GF Filament product page Siraya Tech · 2026-08 · vendor
- ABS / ASA / PC Usage Guide Bambu Lab Wiki · 2026-08 · doc
- ASA — material basics Polymaker Wiki · 2026-08 · doc
- ASA — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- Prusament PETG Technical Datasheet v1.1 Prusa Polymers · 2022-02 · tds
- PETG — material basics Polymaker Wiki · 2026-08 · doc
- Max volumetric speed Prusa Knowledge Base · 2026-08 · doc
- Composite materials filled with carbon, kevlar or glass Prusa Knowledge Base · 2026-08 · doc
- PET and PETG — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- Bambu Filament Technical Data Sheet V3.0 — ASA Bambu Lab · 2026-08 · tds
- PolyLite ASA Technical Data Sheet Polymaker · 2024-11 · tds
- Prusament ASA Technical Datasheet v1.1 Prusa Polymers · 2024-05 · tds
- Wet Filament — signs, causes and drying Polymaker Wiki · 2026-08 · doc
- Extrudr PETG vs PCTG vs XPETG-CF — results spreadsheet My Tech Fun (Igor Gaspar) · 2026-08 · test
- Prusament PETG-CF vs PETG V0 vs PETG — results spreadsheet My Tech Fun (Igor Gaspar) · 2026-08 · test
- BambuLab PETG Basic vs Translucent vs PETG-CF — results spreadsheet My Tech Fun (Igor Gaspar) · 2026-08 · test
- Mechanical Properties of Additively Manufactured Polymeric Materials — PLA and PETG — For Biomechanical Applications Polymers 16(13):1868 · 2024-06 · paper
- Prusament ASA — material page Prusa Polymers · 2026-08 · doc
- Effects of Fiber Orientation on the Coefficient of Thermal Expansion of Fiber-Filled Polymer Systems in Large Format Polymer Extrusion-Based Additive Manufacturing Materials 15(8):2764 · 2022-04 · paper
- ASA — FDM Material Data Sheet (includes 1000 h QUV exposure results) Stratasys · 2026-08 · tds
- Emissions of Ultrafine Particles and Volatile Organic Compounds from Commercially Available Desktop Three-Dimensional Printers with Multiple Filaments (Azimi et al.) Environmental Science & Technology 50(3) 1260-1268 · 2016-01 · paper
- Chemical resistance — resistance of Ensinger plastics to chemicals (DIN 50 014, 23/50) Ensinger · 2026-08 · tds
- Eastman Spectar copolyester — Chemical resistance (unstressed bars, 1 year at 23 °C) Eastman Chemical Company · 2026-08 · tds
- Improve your 3D prints with chemical smoothing Prusa Research · 2026-08 · doc
- HIPS — Knowledge Base Prusa Research · 2026-08 · doc