Filament comparison
ASA-GF vs PEBA
Compare printing settings, strength, heat resistance, dated prices and sources.
2 selected · all documented properties
| Property | Glass-fibre ASA (ASA-GF)ASA | PEBA (polyether block amide)FLEX |
|---|---|---|
| Market snapshot | ||
| Listing priceUSD/kg; dated snapshots | $29.95/kg median; $26.99–$33.99/kg across 3 dated product listings | $60.99/kg median; $60.99–$60.99/kg across 1 dated product listings |
| Identity & Market | ||
| Base polymer / chemistry | ASA reinforced with chopped glass fibre — 10 wt% (Spectrum ASA-X GF10), 15 wt% (ZYLtech ASA-GF)[1][2] | Polyether block amide: rigid polyamide and flexible polyether blocks.[3] |
| Densityg/cm³ | 1.07 (ZYLtech) and 1.11 (Spectrum), ISO 1183[1][2] | 1.01 g/cm³ (GB/T 1033; eSUN manufacturer data)[3] |
| Typical priceUSD/kg | 1 kg spools cluster near 28[4][5] | Not documented |
| Price range across brandsUSD/kg | 27–34 across brands; Ambrosia 27, ZYLtech 30, Siraya Tech 34[4][5][6] | Not documented |
| Market availability1–5 | Niche, a handful of specialist brands[4][1][2] | Not documented |
| Spool sizes & diameters | 1.75 and 2.85 mm; 1 kg spools[2][4] | 1.75 mm diameter, 1 kg spool.[7] |
| Typical applications | Outdoor brackets and mounts that need stiffness and dimensional stability under sun and moisture[1][2] | Manufacturer applications include footwear, sports equipment and cushioning.[3] |
| Diameter tolerance± mm | ±0.01 at 95 % probability and ±0.02 at 100 % (ZYLtech)[2] | Not documented |
| Printing Parameters | ||
| Nozzle temperature°C | 240–270 (Spectrum); 240–280 (ZYLtech)[1][2] | 230–260 °C; 240 °C recommended.[3] |
| Bed temperature°C | 80–100 (Spectrum); 90–110 on PEI (ZYLtech)[1][2] | 60–90 °C[3] |
| Enclosure / chamber requirement1–5 | Enclosure recommended[8] | Not documented |
| Part cooling fan | 0–20 % (Spectrum)[1] | 10–50% fan recommended; mechanical-test specimens used 50–100%.[3] |
| Bed surface & adhesion aid | PEI sheet, BuildTak or an adhesion aid such as Magigoo (Polymaker); Simplify3D also lists Kapton tape and ASA slurry[9][10] | PEI build plate[3] |
| Maximum volumetric flow (mm³/s; see test conditions)mm³/s | 2.4–5.6 at Spectrum's 30–70 mm/s on a 0.4 mm nozzle at 0.2 mm layer; ZYLtech allows up to 200 mm/s[1][2][11] | 9 mm³/s maximum in eSUN spiral-vase test; mechanical specimens used 2 mm³/s. Linear recommendation 25–110 mm/s is a separate quantity.[3] |
| Warping tendency1–5 | Moderate — needs adhesion aid or draught shield[8] | Not documented |
| Bed-adhesion difficulty1–5 | Needs a specific surface plus adhesive[9] | Not documented |
| Stringing / oozing tendency1–5 | Slight — Polymaker advises 1–2 mm retraction at 20–30 mm/s[9] | Not documented |
| Overall printing difficulty1–5 | Intermediate — dry filament and a tuned profile; ZYLtech requires a hardened nozzle of 0.6 mm or larger[2][1] | Not documented |
| Extruder requirement | ZYLtech specifies a hardened nozzle 0.6 mm or larger; Spectrum bases its settings on a 0.5 mm nozzle[2][1] | Not documented |
| Hardware Wear & Reliability | ||
| Nozzle hardness required1–4 | Hardened steel required — Spectrum recommends ruby or hardened, ZYLtech requires hardened[1][2] | Not documented |
| Abrasiveness1–5 | Highly abrasive — standard GF composite[1][2] | Not documented |
| Nozzle clog risk1–5 | Moderate — needs dry filament and a clean nozzle; Prusa lists higher risk of nozzle clogging for glass-filled composites[12] | Not documented |
| Heat-creep / jam sensitivity1–5 | Slightly sensitive[10] | Not documented |
| Hotend requirement | No special hotend required[10] | Not documented |
| Moisture Behaviour | ||
| Moisture absorption (hygroscopicity)1–5 | Moderate — the ASA matrix takes up 0.40–0.45 % saturated at 25 °C / 55 % RH; no glass-filled grade publishes its own figure[13][14][15] | Not documented |
| Drying temperature & time | Not documented | 70–75 °C for 6–8 h; re-dry after receiving or extended exposure.[3] |
| Symptoms when wet | Bubbling and popping at the nozzle, stringing and a rough surface[16] | Not documented |
| Effect of moisture on strength | No dry-versus-conditioned figures are published; Polymaker groups the styrenics as moderate-sensitivity and absorbed water shows as bubbling and poor layer adhesion[16] | Not documented |
| Storage requirement | Sealed with desiccant; Polymaker rates the styrenics moderate-sensitivity[16] | Not documented |
| Mechanical Properties | ||
| Tensile strength (XY)MPa | 33–36 at break, ISO 527 (ZYLtech; specimen type not stated); Spectrum quotes 55 at break on injection-moulded specimens[2][1] | >16.5 MPa printed XY, GB/T 1040; manufacturer lower bound, not an exact measurement.[3] |
| Young's modulusMPa | 2540–2890 (ZYLtech; specimen type not stated) and 2550 (Spectrum, injection-moulded), ISO 527[2][1] | Not documented |
| Elongation at break% | 3.4 at break (ZYLtech; specimen type not stated); Spectrum quotes 2.80 at yield on injection-moulded specimens[2][1] | >520% printed XY, GB/T 1040; manufacturer lower bound.[3] |
| Flexural modulusMPa | 2130–2480 flexural modulus, ISO 178 (ZYLtech; specimen type not stated)[2] | Not documented |
| Charpy impact, notchedkJ/m² | 8.3 notched Charpy at 23 °C on injection-moulded specimens (Spectrum, ISO 179-1eA); ZYLtech publishes notched Izod 6.9 by ISO 180 instead[1][2] | Not documented |
| Other impact data | Charpy unnotched 25 kJ/m² at 23 °C on injection-moulded specimens (Spectrum, ISO 179-1eU); ZYLtech notched Izod 6.9 kJ/m² (ISO 180)[1][2] | Not documented |
| Layer adhesion / Z tensileMPa | Not documented | 7.5 MPa printed Z, GB/T 1040 (manufacturer test)[3] |
| Brittleness1–5 | Brittle — snaps with little warning; elongation at break 3.4 %[2] | Not documented |
| Hardness (scale-specific)Shore A / Shore D / Rockwell | Not documented | 90 Shore A nominal grade designation; do not compare numerically with Shore D or Rockwell.[7] |
| Creep resistance / sustained load1–5 | Good — no creep test found; chopped glass fibre lifts modulus to 2540–2890 against 2379–2450 for unfilled ASA[2][14][13] | Not documented |
| Fatigue / repeated-flex resistance1–5 | Below average — no GF-grade S-N curve; elongation at break falls to 3.4 % against 6.7–9.2 % for unfilled ASA[2][14][13] | Not documented |
| Elasticity / flexibility1–5 | Rigid[2] | Not documented |
| Thermal Properties | ||
| HDT at 0.45 MPa°C | 100 (Spectrum, injection-moulded, ISO 75 at 0.45 MPa)[1] | Not documented |
| HDT at 1.8 MPa°C | 97–99 unannealed (ZYLtech, ISO 75 at 1.8 MPa; specimen type not stated); Spectrum 90 on injection-moulded specimens[2][1] | Not documented |
| Melting point / Vicat°C | Amorphous ASA matrix; Vicat 98 (Spectrum, ISO 306). ZYLtech quotes a 210–220 °C melting range by ISO 11357 for its grade[1][2] | 110 °C Vicat softening (GB/T 1633, 120 °C/h, 10 N); not HDT or a continuous-use rating.[3] |
| Continuous service temperature°C | 93 — Prusa publishes this as the temperature resistance of Prusament ASA[17] | Not documented |
| Flammability / UL 94 | Flammable; no UL 94 rating published[13] | Not documented |
| Environment & Chemical | ||
| UV resistance1–5 | Excellent — designed for permanent outdoor use; Spectrum states the parts resist prolonged UV and moisture exposure[1][18] | Not documented |
| Chemical resistance | Good against weak acids, weak alkalis, oils and grease; dissolved by acetone[14] | Not documented |
| Food contact | Not food safe[9] | Not documented |
| Biodegradability / compostability | Not biodegradable[9] | Not documented |
| Recyclability | Not accepted in household plastic collection[9] | Not documented |
| Health & Safety | ||
| Fume toxicity1–5 | High — hazardous VOC such as styrene; enclosure and filtration needed[19][8] | Not documented |
| Hazardous species emitted | Styrene. Bambu Lab states ABS and ASA release harmful gases such as styrene at printing temperature, which can be toxic and cause dizziness or nausea. Azimi et al. measured styrene from every styrenic filament tested but did not test ASA itself[8][19] | Not documented |
| Ventilation / filtration requirement1–5 | Enclosure with carbon and HEPA filtration[19][8] | Not documented |
| Dust & fibre handling hazard | Glass fibre is bound in the matrix; avoid inhaling sanding dust[1] | Not documented |
| Post-Processing | ||
| Sanding & machining | Sands well and takes filler before painting[9] | Not documented |
| Painting & finishing | Paints readily; ASA holds colour outdoors so many parts are left unpainted[9] | Not documented |
| Gluing & solvent welding | Solvent-welds with acetone[14] | Not documented |
| Vapour / chemical smoothing | Acetone vapour smoothing works[14] | Not documented |
| Support material pairing | HIPS breaks away or dissolves in d-limonene; Bambu Lab sells a Support for ABS that also serves ASA[8] | Not documented |
| Solvents & Solubility | ||
| Soluble in | Acetone dissolves the resin and leaves the fibre; MEK, THF, ethyl acetate and chlorinated solvents attack the styrenic backbone.[20][14] | Not documented |
| Softened or crazed by | Limonene attacks some grades — Prusa reports Prusament ASA Orange flaking apart as layer adhesion fails.[21] | Not documented |
| Solvent welding & smoothing agent | Acetone vapour reaches only the resin fraction, so the fibre is left standing proud of the smoothed surface.[22][14] | Not documented |
Material entries describe families or representative grades, not an interchangeable specification for every spool. Test methods, orientations and conditions may differ. Unknown values are marked “Not documented”. Prices and source dates remain historical snapshots; check the linked guide for product details. Differences highlight text, not a universal winner.
Sources for this comparison
- Spectrum ASA-X GF10 Technical Data Sheet (mechanical and thermal data marked injection-moulded) Spectrum Filaments · 2026-08 · tds
- ZYLtech ASA-GF Filament Technical Data Sheet v1 ZYLtech · 2026-08 · tds
- eSUN PEBA-90A Technical Data Sheet v1.0 (Aug 2025), checked 2026-10-17 eSUN · 2025-08 · tds
- Filastruder product catalogue Filastruder · 2026-08 · vendor
- ZYLtech ASA-GF Glass Fiber filament — product page ZYLtech · 2026-08 · vendor
- Siraya Tech Fibreheart ASA-GF Filament product page Siraya Tech · 2026-08 · vendor
- eSUN PEBA-90A official product page: 1 kg price and product identity eSUN · 2026-10-17 · vendor
- ABS / ASA / PC Usage Guide Bambu Lab Wiki · 2026-08 · doc
- ASA — material basics Polymaker Wiki · 2026-08 · doc
- ASA — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- Max volumetric speed Prusa Knowledge Base · 2026-08 · doc
- Composite materials filled with carbon, kevlar or glass Prusa Knowledge Base · 2026-08 · doc
- Bambu Filament Technical Data Sheet V3.0 — ASA Bambu Lab · 2026-08 · tds
- PolyLite ASA Technical Data Sheet Polymaker · 2024-11 · tds
- Prusament ASA Technical Datasheet v1.1 Prusa Polymers · 2024-05 · tds
- Wet Filament — signs, causes and drying Polymaker Wiki · 2026-08 · doc
- Prusament ASA — material page Prusa Polymers · 2026-08 · doc
- ASA — FDM Material Data Sheet (includes 1000 h QUV exposure results) Stratasys · 2026-08 · tds
- Emissions of Ultrafine Particles and Volatile Organic Compounds from Commercially Available Desktop Three-Dimensional Printers with Multiple Filaments (Azimi et al.) Environmental Science & Technology 50(3) 1260-1268 · 2016-01 · paper
- Chemical resistance — resistance of Ensinger plastics to chemicals (DIN 50 014, 23/50) Ensinger · 2026-08 · tds
- HIPS — Knowledge Base Prusa Research · 2026-08 · doc
- Improve your 3D prints with chemical smoothing Prusa Research · 2026-08 · doc