| Property | Glass-fibre ABS (ABS-GF)ABS | Glass-fibre ASA (ASA-GF)ASA |
|---|---|---|
| Market snapshot | ||
| Listing priceUSD/kg; dated snapshots | $34.99/kg median; $24.49–$73.33/kg across 4 dated product listings | $29.95/kg median; $26.99–$33.99/kg across 3 dated product listings |
| Identity & Market | ||
| Base polymer / chemistry | ABS reinforced with chopped glass fibre — 3DXTech's grade is nominally 10 wt%[1][2] | ASA reinforced with chopped glass fibre — 10 wt% (Spectrum ASA-X GF10), 15 wt% (ZYLtech ASA-GF)[3][4] |
| Densityg/cm³ | 1.08 (Bambu Lab) and 1.15 (3DXTech), ISO 1183[2][1] | 1.07 (ZYLtech) and 1.11 (Spectrum), ISO 1183[3][4] |
| Typical priceUSD/kg | 1 kg-equivalent spools span 24–73; the middle of the market is about 35[5][6][7][8] | 1 kg spools cluster near 28[9][10] |
| Price range across brandsUSD/kg | 24–73 across brands; Siraya Tech 24, Bambu Lab 30, SUNLU 40, 3DXTech 73[5][6][7][8] | 27–34 across brands; Ambrosia 27, ZYLtech 30, Siraya Tech 34[9][10][11] |
| Market availability1–5 | Available from several mainstream brands[5][6] | Niche, a handful of specialist brands[9][3][4] |
| Spool sizes & diameters | 1.75 and 2.85 mm; 750 g and 1 kg spools[6][5] | 1.75 and 2.85 mm; 1 kg spools[4][9] |
| Typical applications | Stiff, dimensionally stable enclosure and tooling parts; Bambu Lab notes the fibre blurs layer lines into a matte finish[2] | Outdoor brackets and mounts that need stiffness and dimensional stability under sun and moisture[3][4] |
| Diameter tolerance± mm | Not documented | ±0.01 at 95 % probability and ±0.02 at 100 % (ZYLtech)[4] |
| Printing Parameters | ||
| Nozzle temperature°C | 240–280 (Bambu Lab)[2] | 240–270 (Spectrum); 240–280 (ZYLtech)[3][4] |
| Bed temperature°C | 80–100 (Bambu Lab)[2] | 80–100 (Spectrum); 90–110 on PEI (ZYLtech)[3][4] |
| Enclosure / chamber requirement1–5 | Enclosure recommended — Bambu Lab specifies a 45–60 °C chamber[2][12] | Enclosure recommended[12] |
| Recommended chamber temperature°C | 45–60 (Bambu Lab)[2] | Not documented |
| Part cooling fan | 0–80 % (Bambu Lab)[2] | 0–20 % (Spectrum)[3] |
| Bed surface & adhesion aid | Clean the plate and apply glue; Simplify3D also lists Kapton tape and ABS slurry[12][13] | PEI sheet, BuildTak or an adhesion aid such as Magigoo (Polymaker); Simplify3D also lists Kapton tape and ASA slurry[14][15] |
| Maximum volumetric flow (mm³/s; see test conditions)mm³/s | 14 at Bambu Lab's 180 mm/s cap on a 0.4 mm nozzle at 0.2 mm layer[2][16] | 2.4–5.6 at Spectrum's 30–70 mm/s on a 0.4 mm nozzle at 0.2 mm layer; ZYLtech allows up to 200 mm/s[3][4][16] |
| Warping tendency1–5 | Moderate — needs adhesion aid or draught shield; Bambu Lab positions the fibre as reducing warping[2] | Moderate — needs adhesion aid or draught shield[12] |
| Bed-adhesion difficulty1–5 | Needs a specific surface plus adhesive[12] | Needs a specific surface plus adhesive[14] |
| Stringing / oozing tendency1–5 | Slight — Polymaker advises 1–2 mm retraction at 20–30 mm/s[17] | Slight — Polymaker advises 1–2 mm retraction at 20–30 mm/s[14] |
| Overall printing difficulty1–5 | Intermediate — dry filament and a tuned profile; hardened nozzle mandatory[12] | Intermediate — dry filament and a tuned profile; ZYLtech requires a hardened nozzle of 0.6 mm or larger[4][3] |
| Extruder requirement | Not documented | ZYLtech specifies a hardened nozzle 0.6 mm or larger; Spectrum bases its settings on a 0.5 mm nozzle[4][3] |
| Hardware Wear & Reliability | ||
| Nozzle hardness required1–4 | Hardened steel required[12] | Hardened steel required — Spectrum recommends ruby or hardened, ZYLtech requires hardened[3][4] |
| Abrasiveness1–5 | Highly abrasive — standard GF composite[12] | Highly abrasive — standard GF composite[3][4] |
| Nozzle clog risk1–5 | Moderate — needs dry filament and a clean nozzle; 3DXTech specifies a hardened 0.4 mm minimum nozzle and 0.25 mm layers or higher for the glass-filled grade[18][19] | Moderate — needs dry filament and a clean nozzle; Prusa lists higher risk of nozzle clogging for glass-filled composites[19] |
| Heat-creep / jam sensitivity1–5 | Slightly sensitive[13] | Slightly sensitive[15] |
| Hotend requirement | No special hot-end required[13] | No special hotend required[15] |
| Moisture Behaviour | ||
| Moisture absorption (hygroscopicity)1–5 | Moderate — 0.53 % saturated at 25 °C / 55 % RH (Bambu Lab)[2] | Moderate — the ASA matrix takes up 0.40–0.45 % saturated at 25 °C / 55 % RH; no glass-filled grade publishes its own figure[20][21][22] |
| Equilibrium moisture content at ~50 % RH% | 0.53 saturated at 25 °C / 55 % RH (Bambu Lab)[2] | Not documented |
| Drying temperature & time | 80 °C for 8 h (Bambu Lab)[2] | Not documented |
| Symptoms when wet | Bubbling and popping at the nozzle, stringing and a rough surface[23] | Bubbling and popping at the nozzle, stringing and a rough surface[23] |
| Effect of moisture on strength | Polymaker rates ABS moderate-sensitivity and publishes no dry-versus-conditioned figures; absorbed water flashes to steam in the hotend and shows as bubbling and poor layer adhesion[23] | No dry-versus-conditioned figures are published; Polymaker groups the styrenics as moderate-sensitivity and absorbed water shows as bubbling and poor layer adhesion[23] |
| Storage requirement | Sealed with desiccant; Polymaker rates ABS moderate-sensitivity[23] | Sealed with desiccant; Polymaker rates the styrenics moderate-sensitivity[23] |
| Mechanical Properties | ||
| Tensile strength (XY)MPa | 36 ± 3 printed XY, ISO 527 (Bambu Lab); 3DXTech quotes 68 at break[2][1] | 33–36 at break, ISO 527 (ZYLtech; specimen type not stated); Spectrum quotes 55 at break on injection-moulded specimens[4][3] |
| Young's modulusMPa | 3160 ± 170 printed XY, ISO 527 (Bambu Lab); 3DXTech quotes 4210[2][1] | 2540–2890 (ZYLtech; specimen type not stated) and 2550 (Spectrum, injection-moulded), ISO 527[4][3] |
| Elongation at break% | 6.3 ± 1.2 printed XY, ISO 527 (Bambu Lab); 3DXTech quotes 2 at break[2][1] | 3.4 at break (ZYLtech; specimen type not stated); Spectrum quotes 2.80 at yield on injection-moulded specimens[4][3] |
| Flexural strengthMPa | 68 ± 4 printed XY, ISO 178 (Bambu Lab); 3DXTech quotes 70[2][1] | Not documented |
| Flexural modulusMPa | 2860 ± 130 printed XY, ISO 178 (Bambu Lab); 3DXTech quotes 4420[2][1] | 2130–2480 flexural modulus, ISO 178 (ZYLtech; specimen type not stated)[4] |
| Charpy impact, notchedkJ/m² | 4.2 ± 1.1 printed XY, ISO 179, notched (Bambu Lab)[2] | 8.3 notched Charpy at 23 °C on injection-moulded specimens (Spectrum, ISO 179-1eA); ZYLtech publishes notched Izod 6.9 by ISO 180 instead[3][4] |
| Other impact data | Charpy unnotched 14.5 ± 1.5 printed XY (Bambu Lab, ISO 179)[2] | Charpy unnotched 25 kJ/m² at 23 °C on injection-moulded specimens (Spectrum, ISO 179-1eU); ZYLtech notched Izod 6.9 kJ/m² (ISO 180)[3][4] |
| Layer adhesion / Z tensileMPa | 29 ± 3 printed Z, ISO 527 (Bambu Lab)[2] | Not documented |
| Brittleness1–5 | Brittle — snaps with little warning; notched Charpy falls from 21.5 to 4.2 kJ/m² against unfilled Bambu Lab ABS[2][24] | Brittle — snaps with little warning; elongation at break 3.4 %[4] |
| Creep resistance / sustained load1–5 | Good — no creep test found; chopped glass fibre lifts modulus to 3160 MPa against 2200 for unfilled Bambu Lab ABS[2][24] | Good — no creep test found; chopped glass fibre lifts modulus to 2540–2890 against 2379–2450 for unfilled ASA[4][21][20] |
| Fatigue / repeated-flex resistance1–5 | Below average — no S-N curve found; notched Charpy falls to 4.2 kJ/m² against 21.5 for unfilled Bambu Lab ABS[2][24] | Below average — no GF-grade S-N curve; elongation at break falls to 3.4 % against 6.7–9.2 % for unfilled ASA[4][21][20] |
| Elasticity / flexibility1–5 | Rigid[2] | Rigid[4] |
| Z strength as % of XY% | 81 (Bambu Lab, printed Z against XY tensile)[2] | Not documented |
| Thermal Properties | ||
| HDT at 0.45 MPa°C | 99 (ISO 75, 0.45 MPa, Bambu Lab) against 87 for unfilled Bambu Lab ABS[2][24] | 100 (Spectrum, injection-moulded, ISO 75 at 0.45 MPa)[3] |
| HDT at 1.8 MPa°C | 88 (ISO 75, 1.8 MPa, Bambu Lab) against 84 for unfilled Bambu Lab ABS[2][24] | 97–99 unannealed (ZYLtech, ISO 75 at 1.8 MPa; specimen type not stated); Spectrum 90 on injection-moulded specimens[4][3] |
| Melting point / Vicat°C | Not documented | Amorphous ASA matrix; Vicat 98 (Spectrum, ISO 306). ZYLtech quotes a 210–220 °C melting range by ISO 11357 for its grade[3][4] |
| Continuous service temperature°C | Not documented | 93 — Prusa publishes this as the temperature resistance of Prusament ASA[25] |
| Flammability / UL 94 | Not documented | Flammable; no UL 94 rating published[20] |
| Environment & Chemical | ||
| UV resistance1–5 | Not documented | Excellent — designed for permanent outdoor use; Spectrum states the parts resist prolonged UV and moisture exposure[3][26] |
| Chemical resistance | Good against weak acids, weak alkalis, oils and grease; dissolved by acetone[27] | Good against weak acids, weak alkalis, oils and grease; dissolved by acetone[21] |
| Food contact | Not food safe — Polymaker cites potential chemical leaching[17] | Not food safe[14] |
| Biodegradability / compostability | Not biodegradable[17] | Not biodegradable[14] |
| Recyclability | Mechanically recyclable but not accepted in household plastic collection[17] | Not accepted in household plastic collection[14] |
| Health & Safety | ||
| Fume toxicity1–5 | High — hazardous VOC such as styrene; enclosure and filtration needed[28][12] | High — hazardous VOC such as styrene; enclosure and filtration needed[28][12] |
| VOC emission rateµg/min | 12–113 styrene, the dominant VOC from every ABS and HIPS combination tested[28] | Not documented |
| Ultrafine-particle emission rateparticles/min | 2 × 10¹⁰ to 9 × 10¹⁰ median across all ABS printers, two orders of magnitude above PLA's ≈1 × 10⁸[28] | Not documented |
| Hazardous species emitted | Styrene dominates. Bambu Lab states ABS and ASA release harmful gases such as styrene at printing temperature, which can be toxic and cause dizziness or nausea[28][12] | Styrene. Bambu Lab states ABS and ASA release harmful gases such as styrene at printing temperature, which can be toxic and cause dizziness or nausea. Azimi et al. measured styrene from every styrenic filament tested but did not test ASA itself[12][28] |
| Ventilation / filtration requirement1–5 | Enclosure with carbon and HEPA filtration — an enclosure alone cut measured UFP by only about 35 %[28][12] | Enclosure with carbon and HEPA filtration[28][12] |
| Dust & fibre handling hazard | Glass fibre is bound in the matrix; avoid inhaling sanding dust[1] | Glass fibre is bound in the matrix; avoid inhaling sanding dust[3] |
| Post-Processing | ||
| Sanding & machining | Sands well and takes filler before painting[17] | Sands well and takes filler before painting[14] |
| Painting & finishing | Paints readily after light abrasion[17] | Paints readily; ASA holds colour outdoors so many parts are left unpainted[14] |
| Gluing & solvent welding | Not documented | Solvent-welds with acetone[21] |
| Vapour / chemical smoothing | Not documented | Acetone vapour smoothing works[21] |
| Support material pairing | HIPS breaks away or dissolves in d-limonene; Bambu Lab sells a dedicated Support for ABS[29][12] | HIPS breaks away or dissolves in d-limonene; Bambu Lab sells a Support for ABS that also serves ASA[12] |
| Dimensional accuracy & detail | Bambu Lab describes a smooth matte finish with micro-spot gloss that blurs layer lines[2] | Not documented |
| Solvents & Solubility | ||
| Soluble in | Acetone dissolves the resin and leaves the fibre as sludge; MEK, THF, ethyl acetate and chlorinated solvents do the same.[30][27] | Acetone dissolves the resin and leaves the fibre; MEK, THF, ethyl acetate and chlorinated solvents attack the styrenic backbone.[30][21] |
| Softened or crazed by | Petrol and perchloroethylene soften it and benzene attacks it; d-limonene disrupts layer adhesion in some ABS and ASA grades.[30][31] | Limonene attacks some grades — Prusa reports Prusament ASA Orange flaking apart as layer adhesion fails.[31] |
| Solvent welding & smoothing agent | Acetone vapour reaches only the resin fraction, so the fibre is left standing proud of the smoothed surface.[32][27] | Acetone vapour reaches only the resin fraction, so the fibre is left standing proud of the smoothed surface.[32][21] |
Material entries describe families or representative grades, not an interchangeable specification for every spool. Test methods, orientations and conditions may differ. Unknown values are marked “Not documented”. Prices and source dates remain historical snapshots; check the linked guide for product details. Differences highlight text, not a universal winner.
Sources for this comparison
- FibreX ABS+GF10 Glass Fiber ABS Technical Data Sheet 3DXTech · 2026-08 · tds
- Bambu Filament Technical Data Sheet V1.0 — ABS-GF Bambu Lab · 2026-08 · tds
- Spectrum ASA-X GF10 Technical Data Sheet (mechanical and thermal data marked injection-moulded) Spectrum Filaments · 2026-08 · tds
- ZYLtech ASA-GF Filament Technical Data Sheet v1 ZYLtech · 2026-08 · tds
- ABS-GF — product page Bambu Lab US Store · 2026-08 · vendor
- 3DXTech product catalogue 3DXTech · 2026-08 · vendor
- Siraya Tech Fibreheart ABS-GF Filament product page Siraya Tech · 2026-08 · vendor
- SUNLU ABS-GF (ABS Glass Fiber) 3D Printer Filament 1 kg SUNLU · 2026-08 · vendor
- Filastruder product catalogue Filastruder · 2026-08 · vendor
- ZYLtech ASA-GF Glass Fiber filament — product page ZYLtech · 2026-08 · vendor
- Siraya Tech Fibreheart ASA-GF Filament product page Siraya Tech · 2026-08 · vendor
- ABS / ASA / PC Usage Guide Bambu Lab Wiki · 2026-08 · doc
- ABS — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- ASA — material basics Polymaker Wiki · 2026-08 · doc
- ASA — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- Max volumetric speed Prusa Knowledge Base · 2026-08 · doc
- ABS — material basics Polymaker Wiki · 2026-08 · doc
- FIBREX ABS+GF — product page (print recommendations) 3DXTech · 2026-08 · doc
- Composite materials filled with carbon, kevlar or glass Prusa Knowledge Base · 2026-08 · doc
- Bambu Filament Technical Data Sheet V3.0 — ASA Bambu Lab · 2026-08 · tds
- PolyLite ASA Technical Data Sheet Polymaker · 2024-11 · tds
- Prusament ASA Technical Datasheet v1.1 Prusa Polymers · 2024-05 · tds
- Wet Filament — signs, causes and drying Polymaker Wiki · 2026-08 · doc
- Bambu Filament Technical Data Sheet V3.0 — ABS Bambu Lab · 2026-08 · tds
- Prusament ASA — material page Prusa Polymers · 2026-08 · doc
- ASA — FDM Material Data Sheet (includes 1000 h QUV exposure results) Stratasys · 2026-08 · tds
- PolyLite ABS Technical Data Sheet (V5.5 served at this URL) Polymaker · 2024-11 · tds
- Emissions of Ultrafine Particles and Volatile Organic Compounds from Commercially Available Desktop Three-Dimensional Printers with Multiple Filaments (Azimi et al.) Environmental Science & Technology 50(3) 1260-1268 · 2016-01 · paper
- HIPS — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- Chemical resistance — resistance of Ensinger plastics to chemicals (DIN 50 014, 23/50) Ensinger · 2026-08 · tds
- HIPS — Knowledge Base Prusa Research · 2026-08 · doc
- Improve your 3D prints with chemical smoothing Prusa Research · 2026-08 · doc