Filament comparison
ASA-GF vs TPU 85A
Compare printing settings, strength, heat resistance, dated prices and sources.
2 selected · all documented properties
| Property | Glass-fibre ASA (ASA-GF)ASA | TPU 85AFLEX |
|---|---|---|
| Market snapshot | ||
| Listing priceUSD/kg; dated snapshots | $29.95/kg median; $26.99–$33.99/kg across 3 dated product listings | $89.89/kg median; $31.99–$106.05/kg across 6 dated product listings |
| Identity & Market | ||
| Base polymer / chemistry | ASA reinforced with chopped glass fibre — 10 wt% (Spectrum ASA-X GF10), 15 wt% (ZYLtech ASA-GF)[1][2] | Soft thermoplastic polyurethane at 82–85 Shore A[3][4][5] |
| Densityg/cm³ | 1.07 (ZYLtech) and 1.11 (Spectrum), ISO 1183[1][2] | 1.11 (BASF Ultrafuse 85A) to 1.19 (NinjaFlex 85A), ISO 1183 / ASTM D792[5][3] |
| Typical priceUSD/kg | 1 kg spools cluster near 28[6][7] | 1 kg-equivalent spools span 32–106; the middle of the market is about 90[8][9][3] |
| Price range across brandsUSD/kg | 27–34 across brands; Ambrosia 27, ZYLtech 30, Siraya Tech 34[6][7][10] | 32–106 across brands; Siraya Tech Flex TPU 85A 32 at 1 kg, add:north TPU Pro Matte 85A 72, Recreus Filaflex 82A 90 at 500 g, Proto-pasta Clear Flexible TPU 90, 3DXTech 3DXFLEX 85A 96, NinjaTek NinjaFlex 106[11][8][9][12][3] |
| Market availability1–5 | Niche, a handful of specialist brands[6][1][2] | Available from several mainstream brands[8][11] |
| Spool sizes & diameters | 1.75 and 2.85 mm; 1 kg spools[2][6] | 1.75, 2.85 and 3 mm; 0.5, 1 and 2 kg spools[8][11][3] |
| Typical applications | Outdoor brackets and mounts that need stiffness and dimensional stability under sun and moisture[1][2] | Soft-touch grips, seals, wearables and anything that must compress and rebound[3][4] |
| Diameter tolerance± mm | ±0.01 at 95 % probability and ±0.02 at 100 % (ZYLtech)[2] | Not documented |
| Printing Parameters | ||
| Nozzle temperature°C | 240–270 (Spectrum); 240–280 (ZYLtech)[1][2] | 200–220 (BASF Ultrafuse 85A, 210 typical)[5] |
| Bed temperature°C | 80–100 (Spectrum); 90–110 on PEI (ZYLtech)[1][2] | 40 (BASF Ultrafuse 85A)[5] |
| Enclosure / chamber requirement1–5 | Enclosure recommended[13] | Open frame is fine[5] |
| Part cooling fan | 0–20 % (Spectrum)[1] | Not documented |
| Bed surface & adhesion aid | PEI sheet, BuildTak or an adhesion aid such as Magigoo (Polymaker); Simplify3D also lists Kapton tape and ASA slurry[14][15] | PEI sheet or painter's tape; Polymaker warns TPU can over-stick and advises a glue stick as a release agent[16][17] |
| Maximum volumetric flow (mm³/s; see test conditions)mm³/s | 2.4–5.6 at Spectrum's 30–70 mm/s on a 0.4 mm nozzle at 0.2 mm layer; ZYLtech allows up to 200 mm/s[1][2][18] | 1.2–3.2 at the 15–40 mm/s BASF specifies on a 0.4 mm nozzle at 0.2 mm layer[5] |
| Warping tendency1–5 | Moderate — needs adhesion aid or draught shield[13] | None[5] |
| Bed-adhesion difficulty1–5 | Needs a specific surface plus adhesive[14] | Sticks to anything — Recreus states its 82A grade has excellent bed adhesion without a heated bed or additives[4] |
| Stringing / oozing tendency1–5 | Slight — Polymaker advises 1–2 mm retraction at 20–30 mm/s[14] | High — drying plus tuning needed[19][17] |
| Overall printing difficulty1–5 | Intermediate — dry filament and a tuned profile; ZYLtech requires a hardened nozzle of 0.6 mm or larger[2][1] | Advanced — enclosure, hardware upgrades, tuning; at this hardness the filament will not push through a Bowden tube[3][4] |
| Extruder requirement | ZYLtech specifies a hardened nozzle 0.6 mm or larger; Spectrum bases its settings on a 0.5 mm nozzle[2][1] | Direct drive only. NinjaTek calls its 85A grade ideal for direct-drive extruders and Recreus specifies direct-drive printers for 82A; BASF caps print speed at 15–40 mm/s with a nozzle of 0.4 mm or larger[3][4][5] |
| Hardware Wear & Reliability | ||
| Nozzle hardness required1–4 | Hardened steel required — Spectrum recommends ruby or hardened, ZYLtech requires hardened[1][2] | Brass fine indefinitely[20] |
| Abrasiveness1–5 | Highly abrasive — standard GF composite[1][2] | Non-abrasive[20] |
| Nozzle clog risk1–5 | Moderate — needs dry filament and a clean nozzle; Prusa lists higher risk of nozzle clogging for glass-filled composites[21] | High — jams from moisture, heat creep or particles[19][17] |
| Heat-creep / jam sensitivity1–5 | Slightly sensitive[15] | Very high — softens in the cold zone readily; soft filament buckles between the drive gear and the melt zone[17][3] |
| Hotend requirement | No special hotend required[15] | No special hot-end required, but a direct-drive extruder is (Simplify3D)[16] |
| Moisture Behaviour | ||
| Moisture absorption (hygroscopicity)1–5 | Moderate — the ASA matrix takes up 0.40–0.45 % saturated at 25 °C / 55 % RH; no glass-filled grade publishes its own figure[22][23][24] | Moderate — NinjaTek measures 0.22 % in 24 h (ASTM D570) and BASF specifies a 70 °C dry for at least 5 h[3][5] |
| Equilibrium moisture content at ~50 % RH% | Not documented | 0.22 after 24 h water immersion (NinjaFlex 85A, ASTM D570) — an immersion figure, not an equilibrium moisture content at 50 % RH[3] |
| Drying temperature & time | Not documented | 70 °C for at least 5 h in a hot-air dryer or vacuum oven (BASF)[5] |
| Symptoms when wet | Bubbling and popping at the nozzle, stringing and a rough surface[19] | Bubbling and popping at the nozzle, stringing and a rough surface[19] |
| Effect of moisture on strength | No dry-versus-conditioned figures are published; Polymaker groups the styrenics as moderate-sensitivity and absorbed water shows as bubbling and poor layer adhesion[19] | Polymaker groups TPU with the highly hygroscopic materials; wet TPU prints with poor layer adhesion and weak, brittle layers[19] |
| Storage requirement | Sealed with desiccant; Polymaker rates the styrenics moderate-sensitivity[19] | Sealed with desiccant; often kept in a dryer during the print[19] |
| Mechanical Properties | ||
| Tensile strength (XY)MPa | 33–36 at break, ISO 527 (ZYLtech; specimen type not stated); Spectrum quotes 55 at break on injection-moulded specimens[2][1] | 26 ultimate (NinjaFlex 85A, ASTM D638)[3] |
| Young's modulusMPa | 2540–2890 (ZYLtech; specimen type not stated) and 2550 (Spectrum, injection-moulded), ISO 527[2][1] | 12 (NinjaFlex 85A, ASTM D638) — two orders of magnitude below any rigid filament; NinjaTek's 95A Cheetah reaches 26 by the same method[3][25] |
| Elongation at break% | 3.4 at break (ZYLtech; specimen type not stated); Spectrum quotes 2.80 at yield on injection-moulded specimens[2][1] | 650 at break (Filaflex 82A) and 660 (NinjaFlex 85A); BASF measures 600 in XY and 320 in ZX[4][3][5] |
| Flexural modulusMPa | 2130–2480 flexural modulus, ISO 178 (ZYLtech; specimen type not stated)[2] | Not documented |
| Charpy impact, notchedkJ/m² | 8.3 notched Charpy at 23 °C on injection-moulded specimens (Spectrum, ISO 179-1eA); ZYLtech publishes notched Izod 6.9 by ISO 180 instead[1][2] | Not documented |
| Other impact data | Charpy unnotched 25 kJ/m² at 23 °C on injection-moulded specimens (Spectrum, ISO 179-1eU); ZYLtech notched Izod 6.9 kJ/m² (ISO 180)[1][2] | Not documented |
| Brittleness1–5 | Brittle — snaps with little warning; elongation at break 3.4 %[2] | Very ductile — bends far before failing[3] |
| Hardness (scale-specific)Shore A / Shore D / Rockwell | Not documented | 29 Shore D / 85 Shore A (BASF Ultrafuse 85A, ISO 7619-1); 85 Shore A (NinjaFlex, ASTM D2240); 82 A nominal for Filaflex[3][5][4] |
| Creep resistance / sustained load1–5 | Good — no creep test found; chopped glass fibre lifts modulus to 2540–2890 against 2379–2450 for unfilled ASA[2][23][22] | Poor — no 85A creep test; a printed 95A TPU bar crept from 74.5 to 82.7 mm over 5 days at 1.25 kg, and softer grades creep more[26] |
| Fatigue / repeated-flex resistance1–5 | Below average — no GF-grade S-N curve; elongation at break falls to 3.4 % against 6.7–9.2 % for unfilled ASA[2][23][22] | Excellent — living hinges viable[17] |
| Elasticity / flexibility1–5 | Rigid[2] | Rubbery / highly elastic[3][4] |
| Z strength as % of XY% | Not documented | 53 — BASF measures 320 % elongation at break in ZX against 600 % in XY[5] |
| Wear resistance & friction | Not documented | Abrasion 0.08 g mass loss over 10 000 cycles (NinjaFlex, ASTM D4060); 82 mm³ (BASF, ISO 4649)[3][5] |
| Thermal Properties | ||
| HDT at 0.45 MPa°C | 100 (Spectrum, injection-moulded, ISO 75 at 0.45 MPa)[1] | Not documented |
| HDT at 1.8 MPa°C | 97–99 unannealed (ZYLtech, ISO 75 at 1.8 MPa; specimen type not stated); Spectrum 90 on injection-moulded specimens[2][1] | Not documented |
| Melting point / Vicat°C | Amorphous ASA matrix; Vicat 98 (Spectrum, ISO 306). ZYLtech quotes a 210–220 °C melting range by ISO 11357 for its grade[1][2] | 216 melting (NinjaFlex 85A, DSC)[3] |
| Continuous service temperature°C | 93 — Prusa publishes this as the temperature resistance of Prusament ASA[27] | Not documented |
| Flammability / UL 94 | Flammable; no UL 94 rating published[22] | Not documented |
| Environment & Chemical | ||
| UV resistance1–5 | Excellent — designed for permanent outdoor use; Spectrum states the parts resist prolonged UV and moisture exposure[1][28] | Good — years with some colour shift; Polymaker lists UV exposure among the conditions TPU withstands[17] |
| Chemical resistance | Good against weak acids, weak alkalis, oils and grease; dissolved by acetone[23] | Withstands industrial solvents and UV exposure (Polymaker)[17] |
| Food contact | Not food safe[14] | Not food safe without specific certification (Polymaker)[17] |
| Biodegradability / compostability | Not biodegradable[14] | Not biodegradable[17] |
| Recyclability | Not accepted in household plastic collection[14] | Not accepted in household plastic collection[17] |
| Health & Safety | ||
| Fume toxicity1–5 | High — hazardous VOC such as styrene; enclosure and filtration needed[29][13] | Low hazard — minimal VOC and particle emission; TPU was not among the nine filaments in the chamber study[29] |
| Hazardous species emitted | Styrene. Bambu Lab states ABS and ASA release harmful gases such as styrene at printing temperature, which can be toxic and cause dizziness or nausea. Azimi et al. measured styrene from every styrenic filament tested but did not test ASA itself[13][29] | Not documented |
| Ventilation / filtration requirement1–5 | Enclosure with carbon and HEPA filtration[29][13] | Open a window / occasional ventilation[29] |
| Dust & fibre handling hazard | Glass fibre is bound in the matrix; avoid inhaling sanding dust[1] | Not documented |
| Post-Processing | ||
| Sanding & machining | Sands well and takes filler before painting[14] | Difficult to sand or smooth; Polymaker limits post-processing to trimming or tumbling[17] |
| Painting & finishing | Paints readily; ASA holds colour outdoors so many parts are left unpainted[14] | Not documented |
| Gluing & solvent welding | Solvent-welds with acetone[23] | Cyanoacrylate bonds TPU; no common solvent welds it[17] |
| Vapour / chemical smoothing | Acetone vapour smoothing works[23] | No practical vapour smoothing[17] |
| Support material pairing | HIPS breaks away or dissolves in d-limonene; Bambu Lab sells a Support for ABS that also serves ASA[13] | Polymaker warns TPU supports are often very difficult to remove[17] |
| Solvents & Solubility | ||
| Soluble in | Acetone dissolves the resin and leaves the fibre; MEK, THF, ethyl acetate and chlorinated solvents attack the styrenic backbone.[30][23] | DMF, DMSO, NMP and THF dissolve TPU; acetone, MEK and cyclohexanone are partial solvents. All laboratory reagents.[31] |
| Softened or crazed by | Limonene attacks some grades — Prusa reports Prusament ASA Orange flaking apart as layer adhesion fails.[32] | Toluene and benzene swell it up to +50 % by weight at 23 °C; esters swell it severely; ethanol and IPA soften it.[31] |
| Solvent welding & smoothing agent | Acetone vapour reaches only the resin fraction, so the fibre is left standing proud of the smoothed surface.[33][23] | None practical — the true solvents (DMF, THF, NMP) are laboratory reagents and leave the joint swollen and weak.[31] |
Material entries describe families or representative grades, not an interchangeable specification for every spool. Test methods, orientations and conditions may differ. Unknown values are marked “Not documented”. Prices and source dates remain historical snapshots; check the linked guide for product details. Differences highlight text, not a universal winner.
Sources for this comparison
- Spectrum ASA-X GF10 Technical Data Sheet (mechanical and thermal data marked injection-moulded) Spectrum Filaments · 2026-08 · tds
- ZYLtech ASA-GF Filament Technical Data Sheet v1 ZYLtech · 2026-08 · tds
- NinjaFlex 85A Technical Specifications NinjaTek · 2026-08 · tds
- Filaflex 82A product page (Shore hardness and elongation) Recreus · 2026-08 · vendor
- Ultrafuse TPU 85A Technical Data Sheet (Version 3.0) BASF Forward AM · 2022-08 · tds
- Filastruder product catalogue Filastruder · 2026-08 · vendor
- ZYLtech ASA-GF Glass Fiber filament — product page ZYLtech · 2026-08 · vendor
- 3DXTech product catalogue 3DXTech · 2026-08 · vendor
- Siraya Tech Flex TPU 85A Filament — product page Siraya Tech · 2026-08 · vendor
- Siraya Tech Fibreheart ASA-GF Filament product page Siraya Tech · 2026-08 · vendor
- Proto-pasta product catalogue Proto-pasta · 2026-08 · vendor
- add:north TPU Pro Matte 85A product page add:north · 2026-08 · vendor
- ABS / ASA / PC Usage Guide Bambu Lab Wiki · 2026-08 · doc
- ASA — material basics Polymaker Wiki · 2026-08 · doc
- ASA — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- Flexible (TPE/TPU) — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- TPU — material basics Polymaker Wiki · 2026-08 · doc
- Max volumetric speed Prusa Knowledge Base · 2026-08 · doc
- Wet Filament — signs, causes and drying Polymaker Wiki · 2026-08 · doc
- Extrudr Product Catalogue (DURAPRO PA12 data block) Extrudr · 2025-03 · tds
- Composite materials filled with carbon, kevlar or glass Prusa Knowledge Base · 2026-08 · doc
- Bambu Filament Technical Data Sheet V3.0 — ASA Bambu Lab · 2026-08 · tds
- PolyLite ASA Technical Data Sheet Polymaker · 2024-11 · tds
- Prusament ASA Technical Datasheet v1.1 Prusa Polymers · 2024-05 · tds
- NinjaTek technical specs comparison chart (Cheetah, NinjaFlex, Armadillo, Alloy 910, Nylon 645) NinjaTek · 2026-08 · tds
- BambuLab TPU 95A HF vs Qidi TPU 95A HF — results spreadsheet My Tech Fun (Igor Gaspar) · 2024-02 · test
- Prusament ASA — material page Prusa Polymers · 2026-08 · doc
- ASA — FDM Material Data Sheet (includes 1000 h QUV exposure results) Stratasys · 2026-08 · tds
- Emissions of Ultrafine Particles and Volatile Organic Compounds from Commercially Available Desktop Three-Dimensional Printers with Multiple Filaments (Azimi et al.) Environmental Science & Technology 50(3) 1260-1268 · 2016-01 · paper
- Chemical resistance — resistance of Ensinger plastics to chemicals (DIN 50 014, 23/50) Ensinger · 2026-08 · tds
- Elastollan — Chemical properties: swelling and chemical resistance BASF · 2026-08 · tds
- HIPS — Knowledge Base Prusa Research · 2026-08 · doc
- Improve your 3D prints with chemical smoothing Prusa Research · 2026-08 · doc