Filament comparison
ABS+ vs e-TPU
Compare printing settings, strength, heat resistance, dated prices and sources.
2 selected · all documented properties
| Property | ABS+ / Tough ABSABS | Foaming / expanded TPU (TPU Aero / TPU Air)FLEX |
|---|---|---|
| Market snapshot | ||
| Listing priceUSD/kg; dated snapshots | $26.49/kg median; $15.99–$29.99/kg across 4 dated product listings | $52.05/kg median; $41.99–$85.29/kg across 6 dated product listings |
| Identity & Market | ||
| Base polymer / chemistry | ABS reformulated for lower warping and a higher glass transition; Polymaker's ABS Pro and ABS Max reach Tg 114.9 and 126.3 °C against 101 °C for PolyLite ABS[1][2][3] | Foaming thermoplastic polyurethane — a blowing agent expands the extrudate so the printed Shore hardness can be tuned by flow rate[4] |
| Densityg/cm³ | 1.04 (ABS Pro) and 1.06 (ABS Max), ISO 1183[1][2] | 1.15 filament (Siraya Tech Flex TPU Air) and 1.05 (Roamr TPU Air HR), ISO 1183; the printed part falls to 0.51–0.93 depending on nozzle temperature (ISO 845)[5][6] |
| Typical priceUSD/kg | 1 kg spools cluster near 27[7] | 1 kg-equivalent spools span 42–85; the middle of the market is about 52[8][9][10][11][12][13] |
| Price range across brandsUSD/kg | 16–30 across brands; SUNLU E-ABS 16, Polymaker ABS Pro 25, YXPOLYER ABS Enhanced 28, Polymaker ABS Max 30[7][14][15] | 42–85 across brands; QIDI TPU-Aero 42, Siraya Tech Flex TPU Air 45, Phaetus aeFlex TPU-Aero 49 direct and 40 at West3D, Roamr TPU Air HR 80A 55 at 800 g, Recreus Filaflex Foamy 73 at 750 g, colorFabb varioShore 85 at 700 g[8][9][10][11][12][13][16] |
| Market availability1–5 | Available from several mainstream brands[7] | Available from several mainstream brands — colorFabb, Recreus, QIDI, Phaetus, Siraya Tech and FusRock all sell an active-foaming TPU[4][8][9][10][12][13] |
| Spool sizes & diameters | 1.75 and 2.85 mm; 1 kg spools[7] | 1.75 mm; 0.7, 0.75, 0.8, 1 and 3 kg spools[4][8][10][11][13] |
| Typical applications | Large enclosure and automotive parts where plain ABS warps or softens too early[1][2] | Cushioning, midsoles, insoles and soft-touch parts where the softness needs to vary within one print; Siraya Tech's Roamr line is aimed specifically at printed footwear[4][11] |
| Diameter tolerance± mm | Not documented | 0.03 (Siraya Tech and Roamr, 1.75 mm)[5][6] |
| Printing Parameters | ||
| Nozzle temperature°C | 270–290 (ABS Pro); 270–300 (ABS Max) — 25–35 °C above plain ABS[1][2] | 230–270 (QIDI and Siraya Tech), 220–260 (Roamr); foaming activates near 230 °C and is strongest at the top of the range[4][5][6][12] |
| Bed temperature°C | 120 (ABS Max)[2] | 30–45 (QIDI and Siraya Tech), 35–50 (Roamr) — a hot bed makes the foamed part over-stick[5][6][12] |
| Enclosure / chamber requirement1–5 | Enclosure required (passive)[1][2][17] | Open frame is fine — Roamr states no enclosure is required[4][6] |
| Part cooling fan | Not documented | 100 % — cooling sets the foamed structure quickly (Siraya Tech and Roamr)[5][6] |
| Bed surface & adhesion aid | Clean the plate and apply glue; Simplify3D also lists Kapton tape and ABS slurry[17][18] | PEI sheet or painter's tape; Polymaker warns TPU can over-stick and advises a glue stick as a release agent, and Siraya Tech recommends PVP glue or Magigoo as a release agent on PEI[19][20][5] |
| Maximum volumetric flow (mm³/s; see test conditions)mm³/s | Up to 250 mm/s (ABS Pro) and 200 mm/s (ABS Max), equivalent to 20 and 16 on a 0.4 mm nozzle at 0.2 mm layer[1][2][21] | Up to 12 (Siraya Tech, Flex TPU Air)[10] |
| Warping tendency1–5 | High — enclosure needed for reliable large parts[17] | Not documented |
| Bed-adhesion difficulty1–5 | Needs a specific surface plus adhesive[17] | Not documented |
| Stringing / oozing tendency1–5 | Slight — Polymaker advises 1–2 mm retraction at 20–30 mm/s[22] | Severe — the material expands inside the hot end, so it oozes on travel moves; QIDI states retraction tuning cannot fix it and Siraya Tech advises setting retraction distance and speed to zero[5][12] |
| Overall printing difficulty1–5 | Intermediate — dry filament and a tuned profile; the hotter nozzle rules out PTFE-lined hotends[1][2] | Advanced — enclosure, hardware upgrades, tuning; both density and hardness follow nozzle temperature and flow[4] |
| Extruder requirement | Not documented | Direct drive; the base material is a 92A TPU[4][23] |
| Hardware Wear & Reliability | ||
| Nozzle hardness required1–4 | Brass fine indefinitely[17] | Brass fine indefinitely — Roamr states plainly that no hardened nozzle is needed[24][6] |
| Abrasiveness1–5 | Non-abrasive[17] | Non-abrasive[24] |
| Nozzle clog risk1–5 | Low — unfilled ABS compound; no special hot-end required and clogging is not among the listed drawbacks[18][25] | Not documented |
| Heat-creep / jam sensitivity1–5 | Slightly sensitive[18] | Not documented |
| Hotend requirement | No special hot-end required[18] | No special hot-end required, but a direct-drive extruder is (Simplify3D)[19] |
| Moisture Behaviour | ||
| Moisture absorption (hygroscopicity)1–5 | Moderate — 0.51 % maximum water absorption (ABS Pro)[1] | Moderate[26] |
| Equilibrium moisture content at ~50 % RH% | 0.51 maximum water absorption (Polymaker ABS Pro)[1] | 1.09 water absorption (QIDI TPU-Aero; the standard is not stated)[12] |
| Drying temperature & time | 70 °C for 6 h (ABS Max)[2] | 70–80 °C for 4–6 h; keep below 15 % RH while printing (Siraya Tech, Roamr and QIDI)[5][6][12] |
| Symptoms when wet | Bubbling and popping at the nozzle, stringing and a rough surface[26] | Bubbling and popping at the nozzle, stringing and a rough surface; Siraya Tech adds that moisture wrecks the foaming itself, not only the surface[26][5] |
| Effect of moisture on strength | Polymaker rates ABS moderate-sensitivity and publishes no dry-versus-conditioned figures[26] | Polymaker groups TPU with the highly hygroscopic materials; no dry-versus-conditioned figures are published[26] |
| Storage requirement | Sealed with desiccant; Polymaker rates ABS moderate-sensitivity[26] | Sealed with desiccant; often kept in a dryer during the print[26] |
| Mechanical Properties | ||
| Tensile strength (XY)MPa | 34.9 (ABS Pro) and 35.7 (ABS Max) printed XY, ISO 527[1][2] | Falls with foaming: colorFabb 24 unfoamed and 12 foamed (ISO 527-1A); Siraya Tech 10.3 at break printed at 240 °C down to 3.8 at 270 °C; QIDI 6.81 at break (ISO 527, XY)[4][5][12] |
| Young's modulusMPa | 2330 (ABS Pro) and 2320 (ABS Max) printed XY, ISO 527[1][2] | 50 unfoamed and 40 foamed (colorFabb, ISO 527-1A)[4] |
| Elongation at break% | 6.7 (ABS Max) and 7.3 (ABS Pro) at break, printed XY, ISO 527[1][2] | 465 unfoamed and 450 foamed (colorFabb, ISO 527-1A); Siraya Tech 629 at 240 °C down to 475 at 270 °C; Roamr 760 down to 540; QIDI 576 (ISO 527, XY)[4][5][6][12] |
| Flexural strengthMPa | 60.1 (ABS Pro) and 63.3 (ABS Max) printed XY, ISO 178[1][2] | Not documented |
| Flexural modulusMPa | 2330 (ABS Pro) and 2500 (ABS Max) printed XY, ISO 178[1][2] | 50 unfoamed and 40 foamed flexural modulus (colorFabb, ISO 178)[4] |
| Charpy impact, notchedkJ/m² | 10.5 (ABS Max) and 14.5 (ABS Pro) printed XY, ISO 179, notched[1][2] | Not documented |
| Layer adhesion / Z tensileMPa | 21.9 (ABS Pro) and 25.4 (ABS Max) printed Z, ISO 527[1][2] | Not documented |
| Brittleness1–5 | Tough — absorbs impact, yields before breaking[1][2] | Very ductile — bends far before failing[4] |
| Hardness (scale-specific)Shore A / Shore D / Rockwell | Not documented | Tunable by nozzle temperature: colorFabb 92 Shore A unfoamed; Siraya Tech 78 A printed at 240 °C falling to 63 A at 270 °C, Roamr TPU Air HR 80A 80 A down to 66 A and HR 85A 83 A down to 70 A (ISO 7619)[4][5][6][27] |
| Creep resistance / sustained load1–5 | Moderate — no creep test found; Tg of 115 °C (ABS Pro) and 126 °C (ABS Max) keeps room-temperature service far below softening[1][2] | Poor — no foamed-grade creep test; a printed 95A TPU bar crept from 74.5 to 82.7 mm over 5 days at 1.25 kg[28] |
| Fatigue / repeated-flex resistance1–5 | Moderate — no S-N curve found; 6.7–7.3 % elongation and 10.5–14.5 kJ/m² notched Charpy, below unfilled Bambu Lab ABS[1][2][29] | Excellent — living hinges viable[20] |
| Elasticity / flexibility1–5 | Rigid[1] | Rubbery / highly elastic[4] |
| Z strength as % of XY% | 63 (ABS Pro) and 71 (ABS Max), printed[1][2] | Not documented |
| Thermal Properties | ||
| HDT at 0.45 MPa°C | 106.4 (ABS Pro) and 118.1 (ABS Max), ISO 75 at 0.45 MPa[1][2] | Not documented |
| HDT at 1.8 MPa°C | 101.4 (ABS Pro) and 113.1 (ABS Max), ISO 75 at 1.8 MPa[1][2] | Not documented |
| Glass transition (Tg)°C | 114.9 (ABS Pro) and 126.3 (ABS Max), DSC[1][2] | Not documented |
| Melting point / Vicat°C | Amorphous — no melting point; Vicat 116.1 (ABS Pro) and 127.4 (ABS Max), ISO 306[1][2] | Vicat softening drops as the foam expands: 83 printed at 240 °C to 53 at 270 °C (Siraya Tech, ISO 306); QIDI 70.4[5][12] |
| Annealing response | Not documented | Foaming activates near 230 °C and expands the extrudate about 1.6×; colorFabb advises dropping flow to 60–70 % to realise the weight saving, and Siraya Tech publishes a flow schedule from 85–90 % at 230 °C down to 50–55 % at 270 °C[4][5] |
| Thermal expansion (CTE)µm/m·K | 86–89 for printed unfilled ABS (fibre Bragg grating, 25–50 °C); no grade-specific measurement published[30] | Not documented |
| Environment & Chemical | ||
| UV resistance1–5 | Months outdoors before embrittlement[22] | Good — years with some colour shift; Polymaker lists UV exposure among the conditions TPU withstands[20] |
| Chemical resistance | Good against weak acids, weak alkalis, oils and grease; dissolved by acetone[3] | Withstands industrial solvents and UV exposure (Polymaker)[20] |
| Food contact | Not food safe — Polymaker cites potential chemical leaching[22] | Not food safe without specific certification (Polymaker)[20] |
| Biodegradability / compostability | Not biodegradable[22] | Not biodegradable[20] |
| Recyclability | Mechanically recyclable but not accepted in household plastic collection[22] | Not accepted in household plastic collection[20] |
| Health & Safety | ||
| Fume toxicity1–5 | High — hazardous VOC such as styrene; enclosure and filtration needed[31][17] | Low hazard — minimal VOC and particle emission; TPU was not among the nine filaments in the chamber study[31] |
| VOC emission rateµg/min | 12–113 styrene, the dominant VOC from every ABS and HIPS combination tested[31] | Not documented |
| Ultrafine-particle emission rateparticles/min | 2 × 10¹⁰ to 9 × 10¹⁰ median across all ABS printers, two orders of magnitude above PLA's ≈1 × 10⁸[31] | Not documented |
| Hazardous species emitted | Styrene dominates. Bambu Lab states ABS and ASA release harmful gases such as styrene at printing temperature, which can be toxic and cause dizziness or nausea[31][17] | Not documented |
| Ventilation / filtration requirement1–5 | Enclosure with carbon and HEPA filtration — an enclosure alone cut measured UFP by only about 35 %[31][17] | Open a window / occasional ventilation[31] |
| Post-Processing | ||
| Sanding & machining | Sands well and takes filler before painting[22] | Difficult to sand or smooth; Polymaker limits post-processing to trimming or tumbling[20] |
| Painting & finishing | Paints readily after light abrasion[22] | Not documented |
| Gluing & solvent welding | Not documented | Cyanoacrylate bonds TPU; no common solvent welds it[20] |
| Vapour / chemical smoothing | Acetone vapour smoothing works[3] | No practical vapour smoothing[20] |
| Support material pairing | HIPS breaks away or dissolves in d-limonene; Bambu Lab sells a dedicated Support for ABS[32][17] | Polymaker warns TPU supports are often very difficult to remove[20] |
| Dimensional accuracy & detail | Not documented | Foamed surfaces are matte and textured; holding a consistent hardness means holding the nozzle temperature steady, and the printed density moves by nearly a factor of two across the 230–270 °C window[4][5] |
| Solvents & Solubility | ||
| Soluble in | Acetone dissolves it — the basis of ABS slurry; so do MEK, THF, ethyl acetate, chloroform, dichloromethane and toluene.[33][3] | DMF, DMSO, NMP and THF dissolve TPU; acetone, MEK and cyclohexanone are partial solvents. All laboratory reagents.[34] |
| Softened or crazed by | Petrol and perchloroethylene soften it and benzene attacks it; d-limonene disrupts layer adhesion in some ABS and ASA grades.[33][35] | Toluene and benzene swell it up to +50 % by weight at 23 °C; the foamed wall soaks up esters and alcohols faster still.[34] |
| Solvent welding & smoothing agent | Acetone: about 20 min of vapour at 80 °C over 5 mm of liquid. Prusa measured layer adhesion more than doubled.[36] | None practical — the true solvents (DMF, THF, NMP) are laboratory reagents and leave the joint swollen and weak.[34] |
Material entries describe families or representative grades, not an interchangeable specification for every spool. Test methods, orientations and conditions may differ. Unknown values are marked “Not documented”. Prices and source dates remain historical snapshots; check the linked guide for product details. Differences highlight text, not a universal winner.
Sources for this comparison
- Polymaker ABS Pro Technical Data Sheet V1 (2026-05-29) Polymaker · 2026-05 · tds
- Polymaker ABS Max Technical Data Sheet V1.1 (2026-06-01) Polymaker · 2026-06 · tds
- PolyLite ABS Technical Data Sheet (V5.5 served at this URL) Polymaker · 2024-11 · tds
- varioShore TPU Technical Data Sheet colorFabb · 2026-08 · tds
- Siraya Tech Flex TPU Air Technical Data Sheet Siraya Tech · 2026-08 · tds
- Roamr TPU Air HR 80A Technical Data Sheet Siraya Tech · 2026-08 · tds
- Polymaker product catalogue Polymaker · 2026-08 · vendor
- Recreus product catalogue Recreus · 2026-08 · vendor
- varioShore TPU Natural — product page colorFabb US · 2026-08 · vendor
- Siraya Tech Flex TPU Air Black Filament — lightweight foaming flexible, product page Siraya Tech · 2026-08 · vendor
- Roamr TPU Air HR 80A Filament — product page Siraya Tech · 2026-08 · vendor
- TPU-Aero Lightweight TPU Filament — product page with specification tables QIDI Tech · 2026-08 · vendor
- aeFlex TPU-Aero — active foaming low weight TPU, product page Phaetus · 2026-08 · vendor
- SUNLU E-ABS (Easy ABS) 3D Printer Filament 1 kg SUNLU · 2026-08 · vendor
- YXPOLYER ABS Enhanced product page YXPOLYER · 2026-08 · vendor
- Phaetus aeWorthy TPU-Aero — reseller listing West3D · 2026-08 · vendor
- ABS / ASA / PC Usage Guide Bambu Lab Wiki · 2026-08 · doc
- ABS — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- Flexible (TPE/TPU) — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- TPU — material basics Polymaker Wiki · 2026-08 · doc
- Max volumetric speed Prusa Knowledge Base · 2026-08 · doc
- ABS — material basics Polymaker Wiki · 2026-08 · doc
- NinjaFlex 85A Technical Specifications NinjaTek · 2026-08 · tds
- Extrudr Product Catalogue (DURAPRO PA12 data block) Extrudr · 2025-03 · tds
- Filament Material Guide Prusa Knowledge Base · 2026-08 · doc
- Wet Filament — signs, causes and drying Polymaker Wiki · 2026-08 · doc
- Roamr TPU Air HR 85A Technical Data Sheet Siraya Tech · 2026-08 · tds
- BambuLab TPU 95A HF vs Qidi TPU 95A HF — results spreadsheet My Tech Fun (Igor Gaspar) · 2024-02 · test
- Bambu Filament Technical Data Sheet V3.0 — ABS Bambu Lab · 2026-08 · tds
- Characterization of Thermal Expansion Coefficient of 3D Printing Polymeric Materials Using Fiber Bragg Grating Sensors Materials 17(18):4668 · 2024-09 · paper
- Emissions of Ultrafine Particles and Volatile Organic Compounds from Commercially Available Desktop Three-Dimensional Printers with Multiple Filaments (Azimi et al.) Environmental Science & Technology 50(3) 1260-1268 · 2016-01 · paper
- HIPS — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- Chemical resistance — resistance of Ensinger plastics to chemicals (DIN 50 014, 23/50) Ensinger · 2026-08 · tds
- Elastollan — Chemical properties: swelling and chemical resistance BASF · 2026-08 · tds
- HIPS — Knowledge Base Prusa Research · 2026-08 · doc
- Improve your 3D prints with chemical smoothing Prusa Research · 2026-08 · doc