| Property | Glass-fibre ABS (ABS-GF)ABS | Foaming ASA (ASA Aero)ASA |
|---|---|---|
| Market snapshot | ||
| Listing priceUSD/kg; dated snapshots | $34.99/kg median; $24.49–$73.33/kg across 4 dated product listings | $49.99/kg median; $49.99–$49.99/kg across 1 dated product listings |
| Identity & Market | ||
| Base polymer / chemistry | ABS reinforced with chopped glass fibre — 3DXTech's grade is nominally 10 wt%[1][2] | ASA with a heat-activated blowing agent that expands at the nozzle[3][4] |
| Densityg/cm³ | 1.08 (Bambu Lab) and 1.15 (3DXTech), ISO 1183[2][1] | 0.99 filament (Bambu Lab, ISO 1183); Formfutura's grade reaches 0.33 g/cm³ fully expanded[3][4] |
| Typical priceUSD/kg | 1 kg-equivalent spools span 24–73; the middle of the market is about 35[5][6][7][8] | 1 kg spools cluster near 50[9] |
| Price range across brandsUSD/kg | 24–73 across brands; Siraya Tech 24, Bambu Lab 30, SUNLU 40, 3DXTech 73[5][6][7][8] | 50 at Bambu Lab's 1 kg listing[9] |
| Market availability1–5 | Available from several mainstream brands[5][6] | Niche, a handful of specialist brands[9][4] |
| Spool sizes & diameters | 1.75 and 2.85 mm; 750 g and 1 kg spools[6][5] | 1.75 mm; 1 kg spools[9] |
| Typical applications | Stiff, dimensionally stable enclosure and tooling parts; Bambu Lab notes the fibre blurs layer lines into a matte finish[2] | Drone airframes, RC parts and floating or outdoor applications where mass matters and UV exposure rules out LW-PLA[4] |
| Printing Parameters | ||
| Nozzle temperature°C | 240–280 (Bambu Lab)[2] | 240–280 (Bambu Lab); 220–285 (Formfutura), with foaming activating near 230 °C and peaking between 270 and 285 °C[3][4] |
| Bed temperature°C | 80–100 (Bambu Lab)[2] | 80–90 (Bambu Lab); 50–90 (Formfutura)[3][4] |
| Enclosure / chamber requirement1–5 | Enclosure recommended — Bambu Lab specifies a 45–60 °C chamber[2][10] | Enclosure recommended — Bambu Lab specifies a 45–60 °C chamber[3][10] |
| Recommended chamber temperature°C | 45–60 (Bambu Lab)[2] | 45–60 (Bambu Lab)[3] |
| Part cooling fan | 0–80 % (Bambu Lab)[2] | 0–80 % (Bambu Lab); 0–50 % (Formfutura)[3][4] |
| Bed surface & adhesion aid | Clean the plate and apply glue; Simplify3D also lists Kapton tape and ABS slurry[10][11] | PEI sheet, BuildTak or an adhesion aid such as Magigoo (Polymaker); Simplify3D also lists Kapton tape and ASA slurry[12][13] |
| Maximum volumetric flow (mm³/s; see test conditions)mm³/s | 14 at Bambu Lab's 180 mm/s cap on a 0.4 mm nozzle at 0.2 mm layer[2][14] | 12 at Bambu Lab's 150 mm/s cap on a 0.4 mm nozzle at 0.2 mm layer[3][14] |
| Warping tendency1–5 | Moderate — needs adhesion aid or draught shield; Bambu Lab positions the fibre as reducing warping[2] | Not documented |
| Bed-adhesion difficulty1–5 | Needs a specific surface plus adhesive[10] | Needs a specific surface plus adhesive[12] |
| Stringing / oozing tendency1–5 | Slight — Polymaker advises 1–2 mm retraction at 20–30 mm/s[15] | Slight — Polymaker advises 1–2 mm retraction at 20–30 mm/s[12] |
| Overall printing difficulty1–5 | Intermediate — dry filament and a tuned profile; hardened nozzle mandatory[10] | Advanced — enclosure, hardware upgrades, tuning; flow has to be cut to match the expansion and the density follows nozzle temperature[4][3] |
| Hardware Wear & Reliability | ||
| Nozzle hardness required1–4 | Hardened steel required[10] | Brass fine indefinitely[10] |
| Abrasiveness1–5 | Highly abrasive — standard GF composite[10] | Non-abrasive[10] |
| Nozzle clog risk1–5 | Moderate — needs dry filament and a clean nozzle; 3DXTech specifies a hardened 0.4 mm minimum nozzle and 0.25 mm layers or higher for the glass-filled grade[16][17] | Not documented |
| Heat-creep / jam sensitivity1–5 | Slightly sensitive[11] | Slightly sensitive[13] |
| Hotend requirement | No special hot-end required[11] | No special hotend required[13] |
| Moisture Behaviour | ||
| Moisture absorption (hygroscopicity)1–5 | Moderate — 0.53 % saturated at 25 °C / 55 % RH (Bambu Lab)[2] | High — 0.80 % saturated at 25 °C / 55 % RH, nearly double unfilled Bambu Lab ASA[3][18] |
| Equilibrium moisture content at ~50 % RH% | 0.53 saturated at 25 °C / 55 % RH (Bambu Lab)[2] | 0.80 saturated at 25 °C / 55 % RH (Bambu Lab)[3] |
| Drying temperature & time | 80 °C for 8 h (Bambu Lab)[2] | 80 °C for 8 h (Bambu Lab)[3] |
| Symptoms when wet | Bubbling and popping at the nozzle, stringing and a rough surface[19] | Bubbling and popping at the nozzle, stringing and a rough surface[19] |
| Effect of moisture on strength | Polymaker rates ABS moderate-sensitivity and publishes no dry-versus-conditioned figures; absorbed water flashes to steam in the hotend and shows as bubbling and poor layer adhesion[19] | No dry-versus-conditioned figures are published; Polymaker groups the styrenics as moderate-sensitivity and absorbed water shows as bubbling and poor layer adhesion[19] |
| Storage requirement | Sealed with desiccant; Polymaker rates ABS moderate-sensitivity[19] | Sealed with desiccant; Polymaker rates the styrenics moderate-sensitivity[19] |
| Mechanical Properties | ||
| Tensile strength (XY)MPa | 36 ± 3 printed XY, ISO 527 (Bambu Lab); 3DXTech quotes 68 at break[2][1] | 32 ± 4 printed XY, ISO 527 (Bambu Lab)[3] |
| Young's modulusMPa | 3160 ± 170 printed XY, ISO 527 (Bambu Lab); 3DXTech quotes 4210[2][1] | 2010 ± 260 printed XY, ISO 527 (Bambu Lab)[3] |
| Elongation at break% | 6.3 ± 1.2 printed XY, ISO 527 (Bambu Lab); 3DXTech quotes 2 at break[2][1] | 5.1 ± 1.6 printed XY, ISO 527 (Bambu Lab)[3] |
| Flexural strengthMPa | 68 ± 4 printed XY, ISO 178 (Bambu Lab); 3DXTech quotes 70[2][1] | 58 ± 6 printed XY, ISO 178 (Bambu Lab)[3] |
| Flexural modulusMPa | 2860 ± 130 printed XY, ISO 178 (Bambu Lab); 3DXTech quotes 4420[2][1] | 1510 ± 120 printed XY, ISO 178 (Bambu Lab)[3] |
| Charpy impact, notchedkJ/m² | 4.2 ± 1.1 printed XY, ISO 179, notched (Bambu Lab)[2] | 8.2 ± 1.6 printed XY, ISO 179, notched (Bambu Lab)[3] |
| Other impact data | Charpy unnotched 14.5 ± 1.5 printed XY (Bambu Lab, ISO 179)[2] | Charpy unnotched 32.0 ± 2.5 printed XY (Bambu Lab, ISO 179)[3] |
| Layer adhesion / Z tensileMPa | 29 ± 3 printed Z, ISO 527 (Bambu Lab)[2] | 21 ± 4 printed Z, ISO 527 (Bambu Lab); flexural Z falls to 24 against 58 in XY[3] |
| Brittleness1–5 | Brittle — snaps with little warning; notched Charpy falls from 21.5 to 4.2 kJ/m² against unfilled Bambu Lab ABS[2][20] | Moderate[3] |
| Creep resistance / sustained load1–5 | Good — no creep test found; chopped glass fibre lifts modulus to 3160 MPa against 2200 for unfilled Bambu Lab ABS[2][20] | Below average — no creep test found; the foamed structure drops modulus to 2010 MPa and load is carried by a lower solid fraction[3][18] |
| Fatigue / repeated-flex resistance1–5 | Below average — no S-N curve found; notched Charpy falls to 4.2 kJ/m² against 21.5 for unfilled Bambu Lab ABS[2][20] | Moderate — no foamed-grade S-N curve; unfilled printed ASA holds a fatigue limit at 25 % of tensile strength[3][21] |
| Elasticity / flexibility1–5 | Rigid[2] | Rigid[3] |
| Z strength as % of XY% | 81 (Bambu Lab, printed Z against XY tensile)[2] | 66 by tensile, 41 by flexural (printed, Bambu Lab)[3] |
| Thermal Properties | ||
| HDT at 0.45 MPa°C | 99 (ISO 75, 0.45 MPa, Bambu Lab) against 87 for unfilled Bambu Lab ABS[2][20] | 85 (ISO 75, 0.45 MPa, Bambu Lab) against 100 for unfilled Bambu Lab ASA[3][18] |
| HDT at 1.8 MPa°C | 88 (ISO 75, 1.8 MPa, Bambu Lab) against 84 for unfilled Bambu Lab ABS[2][20] | 78 (ISO 75, 1.8 MPa, Bambu Lab) against 92 for unfilled Bambu Lab ASA[3][18] |
| Continuous service temperature°C | Not documented | 93 — Prusa publishes this as the temperature resistance of Prusament ASA[22] |
| Flammability / UL 94 | Not documented | Flammable; no UL 94 rating published[18] |
| Environment & Chemical | ||
| UV resistance1–5 | Not documented | Excellent — designed for permanent outdoor use; Formfutura states the foaming grade retains ApolloX's UV resistance[4][23] |
| Chemical resistance | Good against weak acids, weak alkalis, oils and grease; dissolved by acetone[24] | Good against weak acids, weak alkalis, oils and grease; dissolved by acetone[25] |
| Food contact | Not food safe — Polymaker cites potential chemical leaching[15] | Not food safe[12] |
| Biodegradability / compostability | Not biodegradable[15] | Not biodegradable[12] |
| Recyclability | Mechanically recyclable but not accepted in household plastic collection[15] | Not accepted in household plastic collection[12] |
| Health & Safety | ||
| Fume toxicity1–5 | High — hazardous VOC such as styrene; enclosure and filtration needed[26][10] | High — hazardous VOC such as styrene; enclosure and filtration needed[26][10] |
| VOC emission rateµg/min | 12–113 styrene, the dominant VOC from every ABS and HIPS combination tested[26] | Not documented |
| Ultrafine-particle emission rateparticles/min | 2 × 10¹⁰ to 9 × 10¹⁰ median across all ABS printers, two orders of magnitude above PLA's ≈1 × 10⁸[26] | Not documented |
| Hazardous species emitted | Styrene dominates. Bambu Lab states ABS and ASA release harmful gases such as styrene at printing temperature, which can be toxic and cause dizziness or nausea[26][10] | Styrene. Bambu Lab states ABS and ASA release harmful gases such as styrene at printing temperature, which can be toxic and cause dizziness or nausea. Azimi et al. measured styrene from every styrenic filament tested but did not test ASA itself[10][26] |
| Ventilation / filtration requirement1–5 | Enclosure with carbon and HEPA filtration — an enclosure alone cut measured UFP by only about 35 %[26][10] | Enclosure with carbon and HEPA filtration[26][10] |
| Dust & fibre handling hazard | Glass fibre is bound in the matrix; avoid inhaling sanding dust[1] | Not documented |
| Post-Processing | ||
| Sanding & machining | Sands well and takes filler before painting[15] | Sands well and takes filler before painting[12] |
| Painting & finishing | Paints readily after light abrasion[15] | Paints readily; ASA holds colour outdoors so many parts are left unpainted[12] |
| Gluing & solvent welding | Not documented | Solvent-welds with acetone[25] |
| Vapour / chemical smoothing | Not documented | Acetone vapour smoothing works[25] |
| Support material pairing | HIPS breaks away or dissolves in d-limonene; Bambu Lab sells a dedicated Support for ABS[27][10] | HIPS breaks away or dissolves in d-limonene; Bambu Lab sells a Support for ABS that also serves ASA[10] |
| Dimensional accuracy & detail | Bambu Lab describes a smooth matte finish with micro-spot gloss that blurs layer lines[2] | Matte, textured surface that hides layer lines; colour lightens as the foaming degree rises, which doubles as a visual density cue[4] |
| Solvents & Solubility | ||
| Soluble in | Acetone dissolves the resin and leaves the fibre as sludge; MEK, THF, ethyl acetate and chlorinated solvents do the same.[28][24] | Acetone dissolves it (Polymaker); MEK, THF, ethyl acetate and the chlorinated solvents dissolve the styrenic backbone.[28][25] |
| Softened or crazed by | Petrol and perchloroethylene soften it and benzene attacks it; d-limonene disrupts layer adhesion in some ABS and ASA grades.[28][29] | Limonene attacks some grades — Prusa reports Prusament ASA Orange flaking apart as layer adhesion fails.[29] |
| Solvent welding & smoothing agent | Acetone vapour reaches only the resin fraction, so the fibre is left standing proud of the smoothed surface.[30][24] | Acetone vapour, ~20 min at 80 °C over 5 mm of liquid; the foamed wall absorbs solvent, so cut the exposure well short.[30] |
Material entries describe families or representative grades, not an interchangeable specification for every spool. Test methods, orientations and conditions may differ. Unknown values are marked “Not documented”. Prices and source dates remain historical snapshots; check the linked guide for product details. Differences highlight text, not a universal winner.
Sources for this comparison
- FibreX ABS+GF10 Glass Fiber ABS Technical Data Sheet 3DXTech · 2026-08 · tds
- Bambu Filament Technical Data Sheet V1.0 — ABS-GF Bambu Lab · 2026-08 · tds
- Bambu Filament Technical Data Sheet V1.0 — ASA Aero Bambu Lab · 2026-08 · tds
- ApolloX Foaming Technical Data Sheet Formfutura · 2025-07 · tds
- ABS-GF — product page Bambu Lab US Store · 2026-08 · vendor
- 3DXTech product catalogue 3DXTech · 2026-08 · vendor
- Siraya Tech Fibreheart ABS-GF Filament product page Siraya Tech · 2026-08 · vendor
- SUNLU ABS-GF (ABS Glass Fiber) 3D Printer Filament 1 kg SUNLU · 2026-08 · vendor
- ASA Aero — product page Bambu Lab US Store · 2026-08 · vendor
- ABS / ASA / PC Usage Guide Bambu Lab Wiki · 2026-08 · doc
- ABS — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- ASA — material basics Polymaker Wiki · 2026-08 · doc
- ASA — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- Max volumetric speed Prusa Knowledge Base · 2026-08 · doc
- ABS — material basics Polymaker Wiki · 2026-08 · doc
- FIBREX ABS+GF — product page (print recommendations) 3DXTech · 2026-08 · doc
- Composite materials filled with carbon, kevlar or glass Prusa Knowledge Base · 2026-08 · doc
- Bambu Filament Technical Data Sheet V3.0 — ASA Bambu Lab · 2026-08 · tds
- Wet Filament — signs, causes and drying Polymaker Wiki · 2026-08 · doc
- Bambu Filament Technical Data Sheet V3.0 — ABS Bambu Lab · 2026-08 · tds
- Mechanical, Fatigue, and Thermal Characterization of ASA, Nylon 12, PC and PC-ABS Manufactured by Fused Filament Fabrication (FFF) Polymers 18(2):302 · 2026-01 · paper
- Prusament ASA — material page Prusa Polymers · 2026-08 · doc
- ASA — FDM Material Data Sheet (includes 1000 h QUV exposure results) Stratasys · 2026-08 · tds
- PolyLite ABS Technical Data Sheet (V5.5 served at this URL) Polymaker · 2024-11 · tds
- PolyLite ASA Technical Data Sheet Polymaker · 2024-11 · tds
- Emissions of Ultrafine Particles and Volatile Organic Compounds from Commercially Available Desktop Three-Dimensional Printers with Multiple Filaments (Azimi et al.) Environmental Science & Technology 50(3) 1260-1268 · 2016-01 · paper
- HIPS — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- Chemical resistance — resistance of Ensinger plastics to chemicals (DIN 50 014, 23/50) Ensinger · 2026-08 · tds
- HIPS — Knowledge Base Prusa Research · 2026-08 · doc
- Improve your 3D prints with chemical smoothing Prusa Research · 2026-08 · doc