Filament comparison
ABS-ESD vs PVA
Compare printing settings, strength, heat resistance, dated prices and sources.
2 selected · all documented properties
| Property | ESD-safe ABSABS | PVA (soluble support)SUPPORT |
|---|---|---|
| Market snapshot | ||
| Listing priceUSD/kg; dated snapshots | $102.50/kg median; $47.00–$166.67/kg across 4 dated product listings | $65.98/kg median; $42.00–$96.00/kg across 5 dated product listings |
| Identity & Market | ||
| Base polymer / chemistry | ABS compounded with a conductive carbon filler for static-dissipative parts[1] | Polyvinyl alcohol — a water-soluble support polymer[2][3] |
| Densityg/cm³ | 1.09 (ISO 1183)[1] | 0.6–0.9 (3DXTech AquaTek, ISO 1183) and 1.13 (Polymaker PolyDissolve S1)[2][3] |
| Typical priceUSD/kg | 1 kg-equivalent spools span 47–167; the middle of the market is about 103[4][5][6] | 1 kg-equivalent spools span 42–96; the middle of the market is about 66[4][7][8][9] |
| Price range across brandsUSD/kg | 47–167 across brands; IEMAI 47, YXPOLYER 65, 3DXTech 140 at 750 g pricing; the EMI-shielding ABS grade runs 167[4][5][6] | 42–96 across brands; IEMAI 3D E-WATER 42, YXPOLYER 55, Reli3D 66 at 500 g, Polymaker PolyDissolve S1 67 at 750 g, 3DXTech AquaTek 96 at 750 g in 1.75 mm[4][7][8][10][9] |
| Market availability1–5 | Niche, a handful of specialist brands[4] | Stocked by most mainstream brands[4][7][8][10][9] |
| Spool sizes & diameters | 1.75 and 2.85 mm; 750 g spools[4] | 1.75 and 2.85 mm; 0.5 and 0.75 kg spools[4][7] |
| Typical applications | Electronics handling fixtures, trays and jigs used around static-sensitive parts[1] | Dissolvable support for PLA, TPU, PVB and PETG — Polymaker names those four for PolyDissolve S1[3] |
| Printing Parameters | ||
| Nozzle temperature°C | Not documented | 215–225 (Polymaker PolyDissolve S1)[3] |
| Bed temperature°C | Not documented | 25–60 (Polymaker PolyDissolve S1)[3] |
| Enclosure / chamber requirement1–5 | Enclosure recommended[11] | Open frame is fine[3] |
| Part cooling fan | Not documented | Part cooling fan required (Simplify3D)[12] |
| Bed surface & adhesion aid | Clean the plate and apply glue; Simplify3D also lists Kapton tape and ABS slurry[11][13] | PEI sheet or painter's tape[12] |
| Maximum volumetric flow (mm³/s; see test conditions)mm³/s | Not documented | 4–12 at Polymaker's 50–150 mm/s on a 0.4 mm nozzle at 0.2 mm layer[3] |
| Warping tendency1–5 | High — enclosure needed for reliable large parts[11] | Not documented |
| Bed-adhesion difficulty1–5 | Needs a specific surface plus adhesive[11] | Sticks to most surfaces[12] |
| Stringing / oozing tendency1–5 | Slight — Polymaker advises 1–2 mm retraction at 20–30 mm/s[14] | Moderate — retraction tuning needed[12] |
| Overall printing difficulty1–5 | Intermediate — dry filament and a tuned profile[11] | Intermediate — dry filament and a tuned profile; PVA is unusable once it has taken up moisture[15][3] |
| Extruder requirement | Not documented | A second extruder or a tool changer; PVA is a support material, not a model material[3] |
| Hardware Wear & Reliability | ||
| Nozzle hardness required1–4 | Hardened steel required[1] | Brass fine indefinitely[3] |
| Abrasiveness1–5 | Moderately abrasive — conductive carbon filler[1] | Non-abrasive[3] |
| Nozzle clog risk1–5 | Low — 3DXTech lists no special nozzle concerns and no minimum layer height for its ESD-ABS, only an 80 °C pre-dry[16] | Very high — frequent jams without careful setup; wet PVA foams and carbonises in the nozzle[15] |
| Heat-creep / jam sensitivity1–5 | Slightly sensitive[13] | High — all-metal hotend and strong cooling needed; Simplify3D warns PVA clogs if the nozzle is left hot while not extruding[12] |
| Hotend requirement | No special hot-end required[13] | No special hot-end required, but the nozzle must not be parked hot[12] |
| Moisture Behaviour | ||
| Moisture absorption (hygroscopicity)1–5 | Moderate — the ABS matrix takes up 0.51–0.65 % saturated at 25 °C / 55 % RH and 3DXTech specifies a 80 °C, 4 h pre-dry[17][18][16] | Very high (>2 %) — Polymaker measures 10.21 % equilibrium water absorption, by far the highest in the dataset[3] |
| Equilibrium moisture content at ~50 % RH% | Not documented | 10.21 equilibrium water absorption (Polymaker PolyDissolve S1)[3] |
| Symptoms when wet | Bubbling and popping at the nozzle, stringing and a rough surface[15] | Bubbling and popping at the nozzle, stringing and a rough surface; with PVA this progresses to clogging[15] |
| Effect of moisture on strength | Polymaker rates ABS moderate-sensitivity and publishes no dry-versus-conditioned figures; absorbed water flashes to steam in the hotend and shows as bubbling and poor layer adhesion[15] | Polymaker groups PVA with nylon as the most moisture-prone class and says it often has to stay in a dryer while printing; there is no published dry-versus-conditioned strength comparison because PVA is not a structural material[15] |
| Storage requirement | Sealed with desiccant; Polymaker rates ABS moderate-sensitivity[15] | Sealed with desiccant at all times; PVA takes up water faster than any other filament here[15][3] |
| Mechanical Properties | ||
| Tensile strength (XY)MPa | 58 at break (printed XY, ISO 527) — the conductive filler raises strength above the unfilled grade's 42[1][19] | Not documented |
| Young's modulusMPa | 2130 (printed XY, ISO 527)[1] | Not documented |
| Elongation at break% | 4 at break (printed XY, ISO 527)[1] | Not documented |
| Flexural strengthMPa | 80 (printed XY, ISO 178)[1] | Not documented |
| Flexural modulusMPa | 2275 (printed XY, ISO 178)[1] | Not documented |
| Brittleness1–5 | Moderate[1] | Not documented |
| Creep resistance / sustained load1–5 | Moderate — no creep test found; Tg of 105 °C keeps room-temperature service far below softening[1] | Poor — deforms under load at room temperature; PVA is not used structurally[2] |
| Fatigue / repeated-flex resistance1–5 | Below average — no S-N curve found; elongation at break 4 %, well below unfilled ABS[1][19] | Poor — fails after a few cycles[2] |
| Elasticity / flexibility1–5 | Rigid[1] | Not documented |
| Wear resistance & friction | Not documented | 3DXTech marks tensile strength, modulus and elongation as not applicable for its PVA support grade — it is not characterised as a structural material[2] |
| Thermal Properties | ||
| Glass transition (Tg)°C | 105 (DSC)[1] | 60 (3DXTech AquaTek, DSC)[2] |
| Continuous service temperature°C | Not documented | Bounded by a glass transition of 60 °C[2] |
| Flammability / UL 94 | Not documented | Flammable; no UL 94 rating published[2] |
| Environment & Chemical | ||
| UV resistance1–5 | Not documented | Degrades within weeks outdoors, and dissolves in rain long before UV matters[3] |
| Chemical resistance | Good against weak acids, weak alkalis, oils and grease; dissolved by acetone[20] | Dissolves in water; unusable in any wet or humid service environment[3][12] |
| Water / humidity resistance in service1–5 | Not documented | Dissolves or disintegrates — by design[3][2] |
| Food contact | Not food safe — Polymaker cites potential chemical leaching[14] | Not offered as a food-contact material[2] |
| Biodegradability / compostability | Not biodegradable[14] | PVA is water-soluble and biodegrades in wastewater treatment, but Simplify3D notes disposal should follow local guidance[12] |
| Recyclability | Mechanically recyclable but not accepted in household plastic collection[14] | Dissolved PVA goes to drain rather than to recycling[12] |
| Electrical & ESD properties | Surface resistance 10⁷–10⁹ ohm/sq, the static-dissipative band (ASTM D257), against above 10¹³ for unfilled ABS[1][19] | Surface resistance above 10^13 ohm/sq (ASTM D257, 3DXTech AquaTek PVA)[2] |
| Health & Safety | ||
| Fume toxicity1–5 | High — hazardous VOC such as styrene; enclosure and filtration needed[21][11] | Low hazard — minimal VOC and particle emission; none of these materials was in the chamber study[21] |
| VOC emission rateµg/min | 12–113 styrene, the dominant VOC from every ABS and HIPS combination tested[21] | Not documented |
| Ultrafine-particle emission rateparticles/min | 2 × 10¹⁰ to 9 × 10¹⁰ median across all ABS printers, two orders of magnitude above PLA's ≈1 × 10⁸[21] | Not documented |
| Hazardous species emitted | Styrene dominates. Bambu Lab states ABS and ASA release harmful gases such as styrene at printing temperature, which can be toxic and cause dizziness or nausea[21][11] | Not documented |
| Ventilation / filtration requirement1–5 | Enclosure with carbon and HEPA filtration — an enclosure alone cut measured UFP by only about 35 %[21][11] | Open a window / occasional ventilation[21] |
| Dust & fibre handling hazard | Conductive carbon filler is bound in the matrix; avoid inhaling sanding dust[1] | Not documented |
| Post-Processing | ||
| Sanding & machining | Sands well and takes filler before painting[14] | Not sanded — it is dissolved away rather than finished[12] |
| Painting & finishing | Paints readily after light abrasion[14] | Not documented |
| Gluing & solvent welding | Not documented | Not applicable — PVA is a sacrificial support[12] |
| Vapour / chemical smoothing | Not documented | Water is the solvent; no vapour smoothing is used[3] |
| Support material pairing | HIPS breaks away or dissolves in d-limonene; Bambu Lab sells a dedicated Support for ABS[22][11] | This is the support material; Polymaker pairs PolyDissolve S1 with PLA, TPU, PVB and PETG[3] |
| Solvents & Solubility | ||
| Soluble in | Acetone dissolves it — the basis of ABS slurry; so do MEK, THF, ethyl acetate, chloroform, dichloromethane and toluene.[23][20] | Water — tap water works cold, warm moving water is faster; 6–12 h typical, changing the water every few hours.[24][25] |
| Softened or crazed by | Petrol and perchloroethylene soften it and benzene attacks it; d-limonene disrupts layer adhesion in some ABS and ASA grades.[23][26] | Nothing else: polyvinyl alcohol resists organic solvents, so an IPA or acetone rinse leaves the support intact.[27] |
| Solvent welding & smoothing agent | Acetone: about 20 min of vapour at 80 °C over 5 mm of liquid. Prusa measured layer adhesion more than doubled.[28] | None — water dissolves PVA rather than welding it, and no solvent gives it a smoothed surface.[24] |
Material entries describe families or representative grades, not an interchangeable specification for every spool. Test methods, orientations and conditions may differ. Unknown values are marked “Not documented”. Prices and source dates remain historical snapshots; check the linked guide for product details. Differences highlight text, not a universal winner.
Sources for this comparison
- 3DXSTAT ESD-ABS Technical Data Sheet 3DXTech · 2026-08 · tds
- AquaTek PVA Water Soluble Support Technical Data Sheet v1.0 3DXTech · 2026-08 · tds
- PolyDissolve S1 Technical Data Sheet V5.4 Polymaker · 2024-11 · tds
- 3DXTech product catalogue 3DXTech · 2026-08 · vendor
- IEMAI ESD-ABS 3D Printing Filament product page IEMAI 3D · 2026-08 · vendor
- YXPOLYER ABS ESD product page YXPOLYER · 2026-08 · vendor
- Polymaker product catalogue Polymaker · 2026-08 · vendor
- YXPOLYER PVA 1 kg — product page YXPOLYER · 2026-08 · vendor
- IEMAI 3D E-WATER water-soluble support filament — store page IEMAI 3D · 2026-08 · vendor
- Reli3D PVA Filament 1.75 mm 500 g Natural — Amazon listing Amazon.com · 2026-08 · vendor
- ABS / ASA / PC Usage Guide Bambu Lab Wiki · 2026-08 · doc
- PVA — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- ABS — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- ABS — material basics Polymaker Wiki · 2026-08 · doc
- Wet Filament — signs, causes and drying Polymaker Wiki · 2026-08 · doc
- 3DXSTAT ESD-ABS — product page (print recommendations) 3DXTech · 2026-08 · doc
- Bambu Filament Technical Data Sheet V3.0 — ABS Bambu Lab · 2026-08 · tds
- Polymaker ABS Pro Technical Data Sheet V1 (2026-05-29) Polymaker · 2026-05 · tds
- 3DXMAX ABS Technical Data Sheet 3DXTech · 2026-08 · tds
- PolyLite ABS Technical Data Sheet (V5.5 served at this URL) Polymaker · 2024-11 · tds
- Emissions of Ultrafine Particles and Volatile Organic Compounds from Commercially Available Desktop Three-Dimensional Printers with Multiple Filaments (Azimi et al.) Environmental Science & Technology 50(3) 1260-1268 · 2016-01 · paper
- HIPS — Ultimate 3D Printing Materials Guide Simplify3D · 2026-08 · doc
- Chemical resistance — resistance of Ensinger plastics to chemicals (DIN 50 014, 23/50) Ensinger · 2026-08 · tds
- PolyDissolve S1 — Polymaker Wiki Polymaker · 2026-08 · doc
- 3DXTech AquaTek PVA product page 3DXTech · 2026-08 · vendor
- HIPS — Knowledge Base Prusa Research · 2026-08 · doc
- Polyvinyl alcohol — KURARAY POVAL application guide Kuraray · 2026-08 · tds
- Improve your 3D prints with chemical smoothing Prusa Research · 2026-08 · doc